What Inconel 718 (N07718) can and cannot do on superalloy standards (astm, ams, gb/t) is fixed by the verified envelope below. Datasheet facts on Inconel 718, and the decision they drive for superalloy standards (astm, ams, gb/t). Nothing else.

Inconel 718 (N07718) is a Inconel alloy rated to 650 °C, stocked for Turbine discs and rings.

Inconel 718 (N07718) carries a verified composition band of Ni 50.0-55.0%, Cr 17.0-21.0%, Nb 4.75-5.50%, Mo 2.80-3.30%, Ti 0.65-1.15%, Al 0.20-0.80%: the range each element must fall in per the governing standard, and the band the mill certificate cites.

What Superalloy Standards (ASTM, AMS, GB/T) means for Inconel 718

Start from the verified triple for Inconel 718: 8.19 g/cm³ density, 650 °C ceiling. On superalloy standards (astm, ams, gb/t) the duty decides, and the duty is rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.

PropertyInconel 718
GradeInconel 718 (N07718)
Density8.19 g/cm³
Max service temp650 °C
Best dutyRotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C
Available formsForging, Wire, Spring Wire, Bar, Plate, Strip
StandardsAMS 5662, AMS 5663, ASTM B637, UNS N07718

Specification signals

Inconel 718 ships against AMS 5662, AMS 5663, ASTM B637, UNS N07718, and those are the callouts a purchase order can cite. The documented applications tell the same story (turbine discs and rings, compressor blades and fasteners), and a duty outside that list deserves a second look before Inconel 718 goes on the order.

  • One Inconel 718 datasheet callout does most of the work on this page: Precipitation-hardenable to 38 HRC. A purchasing audit on the Inconel 718 order checks that line first.

In practice

Drift starts with vague callouts. Paperwork travels with the part.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy standards (astm, ams, gb/t) resolve for Inconel 718?

Inconel 718 ships against AMS 5662, AMS 5663, ASTM B637, UNS N07718, and those are the callouts a purchase order can cite. Drift starts with vague callouts.

What is Inconel 718 best used for?

Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C, which is where this grade’s datasheet numbers are actually verified.

What forms is Inconel 718 available in?

Stocked forms: Forging, Wire, Spring Wire, Bar, Plate, Strip.

What standards does Inconel 718 meet?

AMS 5662, AMS 5663, ASTM B637, UNS N07718 are the standards Inconel 718 is supplied against, each order closed by an EN 10204 3.1 mill test certificate.

When does Inconel 718 stop being the right choice?

The ceiling is 650 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.