Superalloy Standards (ASTM, AMS, GB/T), applied to Waspaloy (N07001): verified numbers first, then the reasoning a specifier applies to Waspaloy. A RAS Thermal reference page on superalloy standards (astm, ams, gb/t).
Waspaloy is a precipitation-hardenable nickel-chromium-cobalt superalloy with exceptional creep-rupture strength at elevated temperatures.
As density anchors from the verified datasheets, Hastelloy X verifies 8.22 g/cm³ with oxidation resistance to 1100 °C, Inconel 625 verifies 8.44 g/cm³ to 980 °C, and L605 is the heaviest stocked grade at 9.13 g/cm³.
What Superalloy Standards (ASTM, AMS, GB/T) means for Waspaloy
Start from the verified triple for Waspaloy: 8.22 g/cm³ density, 870 °C ceiling. On superalloy standards (astm, ams, gb/t) the duty decides, and the duty is turbine discs, rings, shafts and high-temperature fasteners.
| Property | Waspaloy |
|---|---|
| Grade | Waspaloy (N07001) · GB GH4738 |
| Density | 8.22 g/cm³ |
| Max service temp | 870 °C |
| Best duty | Turbine discs, rings, shafts and high-temperature fasteners |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip |
| Standards | AMS 5708, AMS 5709, AMS 5544, ASTM B637 |
Specification signals
Waspaloy ships against AMS 5708, AMS 5709, AMS 5544, ASTM B637 (GB GH4738), and those are the callouts a purchase order can cite. The documented applications tell the same story (turbine discs and rings, compressor shafts), and a duty outside that list deserves a second look before Waspaloy goes on the order.
- One Waspaloy datasheet callout does most of the work on this page: Precipitation-hardenable for turbine applications. A purchasing audit on the Waspaloy order checks that line first.
In practice
Cite the standard and the UNS together. A designation without its document is how certificates and drawings drift apart. That is the compliance spine under turbine discs, rings, shafts and high-temperature fasteners.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy standards (astm, ams, gb/t) resolve for Waspaloy?
Those documents are the grade’s spine. Pair the designation with its document on the order, and the mill returns a certificate that can be checked line by line.
What is Waspaloy best used for?
Turbine discs, rings, shafts and high-temperature fasteners, which is where this grade’s datasheet numbers are actually verified.
What forms is Waspaloy available in?
Waspaloy ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, within the stock range of each form.
What standards does Waspaloy meet?
Waspaloy ships against AMS 5708, AMS 5709, AMS 5544, ASTM B637 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Waspaloy stop being the right choice?
Waspaloy stops being right above 870 °C, or in media its family was not built for.