What 4J29 can and cannot do on superalloy tensile strength, yield and elongation is fixed by the verified envelope below. Datasheet facts on 4J29, and the decision they drive for superalloy tensile strength, yield and elongation. Nothing else.

4J29 is a Precision alloy rated to 450 °C, stocked for Transistor and IC hermetic packages.

For reference, the precision-alloy anchors are 4J36 (Invar 36) at a near-zero expansion coefficient of about 1.3 × 10⁻⁶/°C from cryogenic to 230 °C, and 1J22 at the highest saturation induction of any commercial soft magnetic material, 2.4 T.

What Superalloy Tensile Strength, Yield and Elongation means for 4J29

4J29 on superalloy tensile strength, yield and elongation: density 8.17 g/cm³, verified ceiling 450 °C. The deciding facts are temperature, media and form, and they land on glass-to-metal and ceramic-to-metal seals in electronic packages.

Property4J29
Grade4J29
Density8.17 g/cm³
Max service temp450 °C
Best dutyGlass-to-metal and ceramic-to-metal seals in electronic packages
Available formsWire, Strip, Bar & Rod, Plate & Sheet
StandardsASTM F15, GB/T 14986, MIL-I-23011

Specification signals

For 4J29, the verified reference data define the strength envelope by condition rather than by a single headline number. In practice the applications list confirms the fit: 4J29 is specified for transistor and ic hermetic packages and microwave tube windows, not as a universal filler.

  • The feature that separates 4J29 from its nearest neighbours is specific: Good plating and brazing. Hold the 4J29 certificate to proving it, not asserting it.

In practice

The certificate, not the datasheet, states the actual tensile, yield and elongation of your heat. That is the number to design against. Name the state, close the deal.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy tensile strength, yield and elongation resolve for 4J29?

4J29 publishes its strength by condition. That is the honest form, because aged, annealed and cold-worked states differ materially. The EN 10204 3.1 route closes the gap: heat-specific chemistry plus the stated condition proves the envelope.

What is 4J29 best used for?

4J29 is stocked for glass-to-metal and ceramic-to-metal seals in electronic packages; the documented edge is that the Kovar expansion alloy whose expansion matches borosilicate glass for hermetic seals.

What forms is 4J29 available in?

Stocked forms: Wire, Strip, Bar & Rod, Plate & Sheet.

What standards does 4J29 meet?

Every 4J29 order cites its governing standard (ASTM F15, GB/T 14986, MIL-I-23011) and arrives with an EN 10204 3.1 certificate proving the heat.

When does 4J29 stop being the right choice?

The ceiling is 450 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.