Superalloy Tensile Strength, Yield and Elongation, applied to Hastelloy C-276 (N10276): verified numbers first, then the reasoning a specifier applies to Hastelloy C-276. A RAS Thermal reference page on superalloy tensile strength, yield and elongation.

Hastelloy C-276 is a nickel-molybdenum-chromium alloy for aggressive wet-corrosion service.

Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0%, W 3.0-4.5% is the certified band for Hastelloy C-276 (N10276): every element bounded by the governing standard and proven on the certificate rather than assumed.

What Superalloy Tensile Strength, Yield and Elongation means for Hastelloy C-276

Hastelloy C-276 (N10276) on superalloy tensile strength, yield and elongation: density 8.89 g/cm³, verified ceiling 400 °C. The deciding facts are temperature, media and form, and they land on chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.

PropertyHastelloy C-276
GradeHastelloy C-276 (N10276)
Density8.89 g/cm³
Max service temp400 °C
Best dutyChemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy
Available formsForging, Wire, Plate, Sheet, Strip, Bar, Tube
StandardsASTM B575, ASTM B574, ASTM B564, UNS N10276

Specification signals

Put 790 MPa, 355 MPa and 40% on the same line and Hastelloy C-276 stops being a name and becomes a section size. In practice the applications list confirms the fit: Hastelloy C-276 is specified for chemical reactor internals and flue-gas desulfurization scrubbers, not as a universal filler.

  • The feature that separates Hastelloy C-276 from its nearest neighbours is specific: Wide acid resistance range. Hold the Hastelloy C-276 certificate to proving it, not asserting it.

In practice

Read down the table and the fall from 790 MPa at room temperature is paid for in stages, every intermediate point carrying its own certificate-grade values. Hold the design inside 355 MPa yield and chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy keeps the margin the datasheet promises.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy tensile strength, yield and elongation resolve for Hastelloy C-276?

Put 790 MPa, 355 MPa and 40% on the same line and Hastelloy C-276 stops being a name and becomes a section size. The certificate beats the brochure.

What is Hastelloy C-276 best used for?

Chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy. The general-purpose Ni-Cr-Mo corrosion grade for aggressive wet service, weldable without post-weld heat treatment.

What forms is Hastelloy C-276 available in?

Hastelloy C-276 ships as Forging, Wire, Plate, Sheet, Strip, Bar, Tube, within the stock range of each form.

What standards does Hastelloy C-276 meet?

Every Hastelloy C-276 order cites its governing standard (ASTM B575, ASTM B574, ASTM B564, UNS N10276) and arrives with an EN 10204 3.1 certificate proving the heat.

When does Hastelloy C-276 stop being the right choice?

Hastelloy C-276 stops being right above 400 °C, or in media its family was not built for.