Ask a superalloy tensile strength, yield and elongation question about Hastelloy X (N06002) and the answer lives in the verified reference data Hastelloy X is built to. This is the specification guide to superalloy tensile strength, yield and elongation on Hastelloy X, drawn from RAS Thermal’s superalloy documentation.
Hastelloy X (N06002) is a Hastelloy alloy rated to 1100 °C, stocked for Gas turbine combustion chambers.
For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.
What Superalloy Tensile Strength, Yield and Elongation means for Hastelloy X
For Hastelloy X (N06002), superalloy tensile strength, yield and elongation comes down to the documented envelope: 8.22 g/cm³, 1100 °C ceiling, and a duty best described as gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C.
| Property | Hastelloy X |
|---|---|
| Grade | Hastelloy X (N06002) · GB GH3536 |
| Density | 8.22 g/cm³ |
| Max service temp | 1100 °C |
| Best duty | Gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube |
| Standards | AMS 5536, AMS 5754, ASTM B435, ASTM B572 |
Specification signals
The verified strength line for Hastelloy X reads: Excellent high-temperature strength. In practice the applications list confirms the fit: Hastelloy X is specified for gas turbine combustion chambers and afterburner components, not as a universal filler.
- The feature that separates Hastelloy X from its nearest neighbours is specific: Excellent high-temperature strength. Hold the Hastelloy X certificate to proving it, not asserting it.
In practice
OES chemistry pins the grade, the stated condition pins the strength, and both have to land on the same certificate. That envelope is what gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C draws on.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy tensile strength, yield and elongation resolve for Hastelloy X?
Class first, heat second. A strength envelope is only as good as the certificate behind it. OES chemistry plus the stated condition is the proof.
What is Hastelloy X best used for?
Gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C, which is where this grade’s datasheet numbers are actually verified.
What forms is Hastelloy X available in?
The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube; sizes follow the stock range for the form you pick.
What standards does Hastelloy X meet?
AMS 5536, AMS 5754, ASTM B435, ASTM B572 are the standards Hastelloy X is supplied against, each order closed by an EN 10204 3.1 mill test certificate.
When does Hastelloy X stop being the right choice?
Two things end it: a peak service temperature above 1100 °C, or media outside the family Hastelloy X was built for.