Ask a superalloy tensile strength, yield and elongation question about Incoloy 800 (N08800) and the answer lives in the verified reference data Incoloy 800 is built to. This is the specification guide to superalloy tensile strength, yield and elongation on Incoloy 800, drawn from RAS Thermal’s superalloy documentation.
Incoloy 800 is an iron-nickel-chromium alloy with good strength and oxidation/carburization resistance at high temperatures.
For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.
What Superalloy Tensile Strength, Yield and Elongation means for Incoloy 800
For Incoloy 800 (N08800), superalloy tensile strength, yield and elongation comes down to the documented envelope: 7.94 g/cm³, 1100 °C ceiling, and a duty best described as petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.
| Property | Incoloy 800 |
|---|---|
| Grade | Incoloy 800 (N08800) · GB NS111 |
| Density | 7.94 g/cm³ |
| Max service temp | 1100 °C |
| Best duty | Petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube |
| Standards | ASTM B163, ASTM B407, ASTM B408, ASME SB-407 |
Specification signals
One line carries the claim. In practice the applications list confirms the fit: Incoloy 800 is specified for ethylene furnace tubes and heat exchanger bundles, not as a universal filler.
- One Incoloy 800 datasheet callout does most of the work on this page: Carburization and nitriding resistant. A purchasing audit on the Incoloy 800 order checks that line first.
In practice
Quoting Good creep-rupture strength without naming the condition leaves the number floating, and a floating number cannot be checked against the heat. That envelope is what petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C draws on.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy tensile strength, yield and elongation resolve for Incoloy 800?
Specification starts from that feature line, Good creep-rupture strength, and ends with a certificate that proves the heat actually reached it. Ask for the condition in writing first, because that is the term that decides whether the certificate reading can match Good creep-rupture strength.
What is Incoloy 800 best used for?
Petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C. The cost-effective Ni-Fe-Cr workhorse for furnace tubes and heat exchangers, oxidation and carburization resistant to 1100 °C.
What forms is Incoloy 800 available in?
The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube; sizes follow the stock range for the form you pick.
What standards does Incoloy 800 meet?
Incoloy 800 ships against ASTM B163, ASTM B407, ASTM B408, ASME SB-407 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Incoloy 800 stop being the right choice?
Two things end it: a peak service temperature above 1100 °C, or media outside the family Incoloy 800 was built for.