Ask a superalloy tensile strength, yield and elongation question about Incoloy 800H (N08810) and the answer lives in the verified reference data Incoloy 800H is built to. This is the specification guide to superalloy tensile strength, yield and elongation on Incoloy 800H, drawn from RAS Thermal’s superalloy documentation.

Incoloy 800H is an alloy supplied against its verified datasheet and the governing standard.

For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.

What Superalloy Tensile Strength, Yield and Elongation means for Incoloy 800H

For Incoloy 800H (N08810), superalloy tensile strength, yield and elongation comes down to the documented envelope: 7.94 g/cm³, 1100 °C ceiling, and a duty best described as ASME pressure vessels, steam methane reformers and power plant superheaters.

PropertyIncoloy 800H
GradeIncoloy 800H (N08810) · GB NS1102
Density7.94 g/cm³
Max service temp1100 °C
Best dutyASME pressure vessels, steam methane reformers and power plant superheaters
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII

Specification signals

The verified strength line for Incoloy 800H reads: Enhanced creep strength vs 800. The documented applications tell the same story (asme pressure vessels, high-temperature heat exchangers), and a duty outside that list deserves a second look before Incoloy 800H goes on the order.

  • The feature that separates Incoloy 800H from its nearest neighbours is specific: Superior to 800 above 600°C. Hold the Incoloy 800H certificate to proving it, not asserting it.

In practice

The condition decides the reading (aged, annealed or cold-worked), so confirm the state on the EN 10204 3.1 certificate rather than quoting the datasheet cold. Which is the strength profile ASME pressure vessels, steam methane reformers and power plant superheaters is designed around.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy tensile strength, yield and elongation resolve for Incoloy 800H?

On strength, Incoloy 800H is specified by its own feature set, and the feature says: Enhanced creep strength vs 800. Treat the datasheet value as the class to hold, and the mill certificate as the evidence that your heat holds it.

What is Incoloy 800H best used for?

ASME pressure vessels, steam methane reformers and power plant superheaters. The controlled-carbon 800 variant with enhanced creep strength for ASME pressure vessel duty above 600 °C.

What forms is Incoloy 800H available in?

The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube; sizes follow the stock range for the form you pick.

What standards does Incoloy 800H meet?

Incoloy 800H ships against ASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Incoloy 800H stop being the right choice?

Two things end it: a peak service temperature above 1100 °C, or media outside the family Incoloy 800H was built for.