Most buyers arriving with a superalloy tensile strength, yield and elongation question about L605 (R30605) need one decision on superalloy tensile strength, yield and elongation, not a survey. The verified L605 data and the routing logic here close it for good.

L605 (R30605) is a Cobalt-Based grade whose datasheet leans on one documented property: Excellent wear and galling resistance.

As density anchors from the verified datasheets, Hastelloy X verifies 8.22 g/cm³ with oxidation resistance to 1100 °C, Inconel 625 verifies 8.44 g/cm³ to 980 °C, and L605 is the heaviest stocked grade at 9.13 g/cm³.

What Superalloy Tensile Strength, Yield and Elongation means for L605

L605 (R30605) on superalloy tensile strength, yield and elongation: density 9.13 g/cm³, verified ceiling 980 °C. The deciding facts are temperature, media and form, and they land on aerospace bearing races, wear rings and combustion hardware.

PropertyL605
GradeL605 (R30605) · GB GH605
Density9.13 g/cm³
Max service temp980 °C
Best dutyAerospace bearing races, wear rings and combustion hardware
Available formsForging, Wire, Bar & Rod
StandardsAMS 5759, AMS 5537, ASTM F90

Specification signals

The verified strength line for L605 reads: Biocompatible (ASTM F90). In practice the applications list confirms the fit: L605 is specified for aerospace bearing races and rings and gas turbine wear components, not as a universal filler.

  • The feature that separates L605 from its nearest neighbours is specific: Non-magnetic. Hold the L605 certificate to proving it, not asserting it.

In practice

Evidence beats assertion. Once the certificate names the state and the values, aerospace bearing races, wear rings and combustion hardware has the strength story it was promised.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy tensile strength, yield and elongation resolve for L605?

On strength, L605 is specified by its own feature set, and the feature says: Biocompatible (ASTM F90). Cold-quoted datasheets lose arguments at goods-in.

What is L605 best used for?

L605 is stocked for aerospace bearing races, wear rings and combustion hardware; the documented edge is that a Co-Cr-W-Ni grade combining wear and galling resistance with oxidation resistance to 980 °C.

What forms is L605 available in?

The stocked forms are Forging, Wire, Bar & Rod; sizes follow the stock range for the form you pick.

What standards does L605 meet?

Every L605 order cites its governing standard (AMS 5759, AMS 5537, ASTM F90) and arrives with an EN 10204 3.1 certificate proving the heat.

When does L605 stop being the right choice?

Two things end it: a peak service temperature above 980 °C, or media outside the family L605 was built for.