Ask a superalloy tensile strength, yield and elongation question about MP35N (R30035) and the answer lives in the verified reference data MP35N is built to. This is the specification guide to superalloy tensile strength, yield and elongation on MP35N, drawn from RAS Thermal’s superalloy documentation.

MP35N (R30035): Co-Ni-Cr-Mo alloy with ultra-high tensile strength, fatigue endurance and biocompatibility..

For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.

What Superalloy Tensile Strength, Yield and Elongation means for MP35N

For MP35N (R30035), superalloy tensile strength, yield and elongation comes down to the documented envelope: 8.43 g/cm³, 425 °C ceiling, and a duty best described as medical implants, aerospace fasteners and high-performance springs.

PropertyMP35N
GradeMP35N (R30035)
Density8.43 g/cm³
Max service temp425 °C
Best dutyMedical implants, aerospace fasteners and high-performance springs
Available formsForging, Wire, Spring Wire, Bar & Rod, Strip
StandardsASTM F562, AMS 5844, AMS 5845, ISO 5832-6

Specification signals

The datasheet makes the promise in one line: Ultra-high tensile strength (>1800 MPa achievable). In practice the applications list confirms the fit: MP35N is specified for medical implants and guidewires and aerospace fasteners, not as a universal filler.

  • The feature that separates MP35N from its nearest neighbours is specific: Seawater corrosion resistant. Hold the MP35N certificate to proving it, not asserting it.

In practice

A strength envelope is only as good as the certificate behind it. OES chemistry plus the stated condition is the proof. Those are the numbers medical implants, aerospace fasteners and high-performance springs has to live within.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy tensile strength, yield and elongation resolve for MP35N?

The verified strength line for MP35N reads: Ultra-high tensile strength (>1800 MPa achievable). Evidence beats assertion.

What is MP35N best used for?

Medical implants, aerospace fasteners and high-performance springs, which is where this grade’s datasheet numbers are actually verified.

What forms is MP35N available in?

MP35N ships as Forging, Wire, Spring Wire, Bar & Rod, Strip, within the stock range of each form.

What standards does MP35N meet?

Every MP35N order cites its governing standard (ASTM F562, AMS 5844, AMS 5845, ISO 5832-6) and arrives with an EN 10204 3.1 certificate proving the heat.

When does MP35N stop being the right choice?

Two things end it: a peak service temperature above 425 °C, or media outside the family MP35N was built for.