Most buyers arriving with a superalloy tensile strength, yield and elongation question about Waspaloy (N07001) need one decision on superalloy tensile strength, yield and elongation, not a survey. The verified Waspaloy data and the routing logic here close it for good.

Waspaloy (N07001): Precipitation-hardenable Ni-Cr-Co alloy for turbine discs, rings and high-temperature fasteners..

As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.

What Superalloy Tensile Strength, Yield and Elongation means for Waspaloy

Start from the verified triple for Waspaloy: 8.22 g/cm³ density, 870 °C ceiling. On superalloy tensile strength, yield and elongation the duty decides, and the duty is turbine discs, rings, shafts and high-temperature fasteners.

PropertyWaspaloy
GradeWaspaloy (N07001) · GB GH4738
Density8.22 g/cm³
Max service temp870 °C
Best dutyTurbine discs, rings, shafts and high-temperature fasteners
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip
StandardsAMS 5708, AMS 5709, AMS 5544, ASTM B637

Specification signals

Waspaloy’s datasheet states its strength envelope directly: Exceptional creep-rupture strength to 870°C. The documented applications tell the same story (turbine discs and rings, compressor shafts), and a duty outside that list deserves a second look before Waspaloy goes on the order.

  • One Waspaloy datasheet callout does most of the work on this page: Precipitation-hardenable for turbine applications. A purchasing audit on the Waspaloy order checks that line first.

In practice

Ask for the condition in writing first, because that is the term that decides whether the certificate reading can match Exceptional creep-rupture strength to 870°C. Those are the numbers turbine discs, rings, shafts and high-temperature fasteners has to live within.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy tensile strength, yield and elongation resolve for Waspaloy?

On strength, Waspaloy is specified by its own feature set, and the feature says: Exceptional creep-rupture strength to 870°C. The condition decides the reading (aged, annealed or cold-worked), so confirm the state on the EN 10204 3.1 certificate rather than quoting the datasheet cold.

What is Waspaloy best used for?

Waspaloy is stocked for turbine discs, rings, shafts and high-temperature fasteners; the documented edge is that a Ni-Cr-Co age-hardenable grade with creep-rupture strength across 650 to 870 °C.

What forms is Waspaloy available in?

Waspaloy ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, within the stock range of each form.

What standards does Waspaloy meet?

Waspaloy ships against AMS 5708, AMS 5709, AMS 5544, ASTM B637 as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Waspaloy stop being the right choice?

The ceiling is 870 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.