4J29 is chosen for one property: its thermal expansion coefficient tracks borosilicate glass and alumina ceramics closely enough to hold a hermetic seal through thermal cycling. Where a seal package leaks, the alloy is rarely wrong, the match between the alloy’s expansion curve and the seal partner’s curve is what was wrong. This page sets out the verified facts a package designer needs.

4J29 (Kovar) is an iron-nickel-cobalt controlled expansion alloy whose thermal expansion coefficient closely matches that of borosilicate glass and alumina ceramics.

What expansion matching means for 4J29

A glass-to-metal or ceramic-to-metal seal survives because the metal and the insulator expand and contract together from the sealing temperature down to service. 4J29 (Kovar) is specified for exactly that duty, the site datasheet lists expansion matching to borosilicate glass as the first key feature, with hermetic seal qualification and leak-tightness to 10⁻⁹ cc He/s as the verified acceptance figures. If your seal partner is not borosilicate glass or alumina ceramic, the match has to be re-proven rather than assumed.

Property4J29 (verified)
Expansion behaviourMatches borosilicate glass and alumina ceramics
Hermetic leak rate10⁻⁹ cc He/s
Max service temperature450 °C
Density8.17 g/cm³
Governing standardsASTM F15, GB/T 14986, MIL-I-23011
Stock formsWire, Strip, Bar & Rod, Plate & Sheet

Specification signals

Seal duty decides the form: strip for pressed lead frames and reed switch blades, wire for matched-diameter feedthrough pins, plate and sheet for package headers and microwave tube windows. Transistor and IC hermetic packages, optoelectronic housings and cryogenic electrical feedthroughs are the listed applications, each one pairs 4J29 with a glass or ceramic partner chosen to ride the same expansion curve.

  • Seal packages: transistor and IC hermetic headers, microwave tube windows, optoelectronic housings
  • Switching: reed switch glass seals, where strip temper and glass wetting decide life
  • Cryogenic feedthroughs: electrical feedthroughs that must stay leak-tight as the package cools

Where 4J29 stops being the answer

Above the 450 °C service ceiling the datasheet guarantee ends, and a seal partner outside the borosilicate-glass / alumina-ceramic set voids the expansion match. 4J29 also is not a magnetic-shielding or structural pick. It is a sealing alloy, and specify it against ASTM F15 or GB/T 14986 with the 10⁻⁹ cc He/s leak criterion written into the purchase order.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

Why does a hermetic seal fail if 4J29 expansion matches the glass?

Matching is a property of the pair, not of the alloy alone. The datasheet verifies the match against borosilicate glass and alumina ceramics, and a different glass family or a hard-soldered joint changes the stress state, and the leak path appears at the interface rather than in the metal.

What leak rate qualifies a 4J29 seal package?

The verified acceptance figure is 10⁻⁹ cc He/s leak-tightness. Write that number and the test method into the drawing so the hermetic criterion is testable, not assumed.

Can 4J29 be used above 450 °C?

No. The verified maximum service temperature is 450 °C. Above that ceiling the datasheet guarantee ends and the expansion match to the seal partner is no longer covered by the grade’s own documentation.

Which standard should a 4J29 purchase order cite?

ASTM F15 is the international sealing-alloy designation, GB/T 14986 the Chinese precision-alloy standard and MIL-I-23011 the military specification. Cite one explicitly, the certificate must prove the grade by chemistry against it.