Expansion matched to borosilicate glass and ceramics, or near-zero expansion for dimensional stability itself?
4J29 (Kovar) is an iron-nickel-cobalt controlled expansion alloy whose thermal expansion coefficient closely matches that of borosilicate glass and alumina ceramics.
Route the decision
- If the part is a hermetic seal, glass-to-metal or ceramic-to-metal in transistor headers, microwave windows, optoelectronic housings, take 4J29 (Kovar): its expansion coefficient matches borosilicate glass and alumina ceramics per ASTM F15, leak-tight to 10⁻⁹ cc He/s.
- If the part must not change size, optical benches, LNG tank membranes, composite tooling, laser cavities, take 4J36 (Invar 36): near-zero thermal expansion of about 1.3 × 10⁻⁶/°C from cryogenic to 230 °C per ASTM F1684.
- If the duty runs above 230 °C, 4J29 is the only one of the pair rated there, its verified envelope reaches 450 °C, while 4J36’s low-expansion behaviour is specified to 230 °C.
- If cryogenic dimensional stability decides, 4J36’s verified range starts at cryogenic temperatures, the LNG-membrane and cryogenic-transfer-lane duty 4J29 does not target.
| Property | 4J29 | 4J36 |
|---|---|---|
| UNS / GB | n/a | n/a |
| Density | 8.17 g/cm³ | 8.1 g/cm³ |
| Max service temp | 450 °C | 230 °C |
| Governing standards | ASTM F15, GB/T 14986, MIL-I-23011 | ASTM F1684, GB/T 14986, AFNOR NF A54-301 |
| Stock forms | Wire, Strip, Bar & Rod, Plate & Sheet | Wire, Strip, Bar & Rod, Plate & Sheet |
Specification signals
4J29 wins the sealing axis: expansion matched to borosilicate glass and alumina ceramics, hermetic-seal qualification, good plating and brazing, the universal glass-to-metal standard under ASTM F15 and MIL-I-23011. 4J36 wins the stability axis: near-zero expansion (about 1.3 × 10⁻⁶/°C) from cryogenic to 230 °C, the Invar champion under ASTM F1684 for optical, LNG and tooling duty.
- 4J29: 4J29 wins the sealing axis: expansion matched to borosilicate glass and alumina ceramics, hermetic-seal qualification, good plating and brazing, the universal glass-to-metal standard under ASTM F15 and MIL-I-23011.
- 4J36: 4J36 wins the stability axis: near-zero expansion (about 1.3 × 10⁻⁶/°C) from cryogenic to 230 °C, the Invar champion under ASTM F1684 for optical, LNG and tooling duty.
Switch triggers
Move 4J36 to 4J29 the moment a hermetic joint to glass or ceramic enters the design, and move 4J29 to 4J36 when no seal exists and the requirement is pure dimensional stability, especially below 230 °C or at cryogenic temperature.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
4J29 or 4J36 for a glass-to-metal seal?
4J29 (Kovar), matching borosilicate glass expansion is its verified core, qualified for hermetic seals under ASTM F15. 4J36 minimises expansion but is not the glass-matching standard.
Which has the lower thermal expansion?
4J36 (Invar 36), at about 1.3 × 10⁻⁶/°C, near-zero against 4J29’s glass-matched coefficient. Lowest expansion and matched expansion are different requirements.
Which runs hotter?
4J29: verified envelope to 450 °C, while 4J36’s low-expansion behaviour is specified from cryogenic to 230 °C.
Can 4J36 replace 4J29 in electronic packages?
Only where no hermetic glass seal is involved. The package standard is Kovar because seal integrity, not minimum expansion, decides, 4J36 does not carry the glass-matching qualification.