Two gamma-prime nickel grades: valve-and-blade duty to 815 °C, or creep-rupture discs and rings to 870 °C?

Nimonic 80A is a precipitation-hardenable nickel-chromium alloy with additions of titanium and aluminum for gamma-prime strengthening.

Route the decision

  • If the part is an exhaust valve, blade or high-temperature spring, automotive, marine diesel, gas turbine, take Nimonic 80A: the classic gamma-prime valve alloy with good hot hardness, serviceable to 815 °C under ASTM B637 and BS HR 201.
  • If the part is a disc, ring or shaft under sustained load, creep-rupture hardware from 650 to 870 °C, take Waspaloy: verified creep-rupture strength across that band, with microstructural stability under cyclic thermal loading, under AMS 5708/5709.
  • If thermal cycling with stability decides, Waspaloy’s verified stability feature is the differentiator, the rotating-disc duty, and Nimonic 80A’s precedent is valve and spring hardware.
  • If the form is precision spring wire, Nimonic 80A lists high-temperature springs among its verified applications, the narrower but deeply proven lane of the two.
PropertyNimonic 80AWaspaloy
UNS / GBN07080N07001
Density8.19 g/cm³8.22 g/cm³
Max service temp815 °C870 °C
Governing standardsASTM B637, BS HR 201, AMS 5763, DIN 17742AMS 5708, AMS 5709, AMS 5544, ASTM B637
Stock formsForging, Wire, Spring Wire, Flange, Bar & Rod, Plate & SheetForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip

Specification signals

Nimonic 80A wins the valve-and-spring axis: sixty years of exhaust-valve precedent, hot hardness verified, 815 °C service, spring and bolting forms stocked, the industry-standard choice under ASTM B637 / BS HR 201. Waspaloy wins the creep axis: verified creep-rupture strength across 650-870 °C is exactly the band above Nimonic 80A’s comfort zone, with AMS 5708/5709 covering the disc, ring and shaft hardware.

  • Nimonic 80A: Nimonic 80A wins the valve-and-spring axis: sixty years of exhaust-valve precedent, hot hardness verified, 815 °C service, spring and bolting forms stocked, the industry-standard choice under ASTM B637 / BS HR 201.
  • Waspaloy: Waspaloy wins the creep axis: verified creep-rupture strength across 650-870 °C is exactly the band above Nimonic 80A’s comfort zone, with AMS 5708/5709 covering the disc, ring and shaft hardware.

Switch triggers

Move Nimonic 80A to Waspaloy when the part becomes a rotating or creep-loaded component above 815 °C, and move Waspaloy to Nimonic 80A when the hardware is a valve, spring or bolt, the load case 80A’s sixty-year failure history already covers.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

Nimonic 80A or Waspaloy for exhaust valves?

Nimonic 80A. It is the verified exhaust-valve industry standard with good hot hardness to 815 °C. Waspaloy’s pedigree is creep-rupture discs and rings, not valve-seat duty.

Which runs hotter?

Waspaloy, at 870 °C verified creep-rupture service against Nimonic 80A’s 815 °C, and the real gap is under sustained load, where Waspaloy’s creep data exist.

Are both precipitation-hardened?

Yes, both are gamma-prime strengthened nickel grades. The separation is duty: valve and spring hardware routes to 80A, creep-loaded rotating hardware routes to Waspaloy.

Which is heavier?

Nearly identical, Nimonic 80A verifies 8.19 g/cm³ and Waspaloy 8.22 g/cm³, so the decision is entirely duty and certification route.