Incoloy 800 (N08800) is a Incoloy alloy rated to 1100 °C, stocked for Ethylene furnace tubes.

As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.

What Superalloy Weldability means for Incoloy 800

For Incoloy 800 (N08800), superalloy weldability comes down to the documented envelope: 7.94 g/cm³, 1100 °C ceiling, and a duty best described as petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.

PropertyIncoloy 800
GradeIncoloy 800 (N08800) · GB NS111
Density7.94 g/cm³
Max service temp1100 °C
Best dutyPetrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B163, ASTM B407, ASTM B408, ASME SB-407

Specification signals

Incoloy 800’s welding guidance is grade-specific. Filler, preheat and post-weld treatment all follow the datasheet. The documented applications tell the same story (ethylene furnace tubes, heat exchanger bundles), and a duty outside that list deserves a second look before Incoloy 800 goes on the order.

  • One Incoloy 800 datasheet callout does most of the work on this page: Cost-effective vs Inconel. A purchasing audit on the Incoloy 800 order checks that line first.

In practice

Choose the filler from the Incoloy 800 guidance, set preheat from the same page, and only then strike the arc. That is the fabrication assumption behind petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy weldability resolve for Incoloy 800?

Filler, heat and after-treatment for Incoloy 800 all come from the datasheet, page by page. Before welding, both heats exist on certificates, and after welding the repair paperwork has to name them both again.

What is Incoloy 800 best used for?

Petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C, which is where this grade’s datasheet numbers are actually verified.

What forms is Incoloy 800 available in?

Incoloy 800 ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube, within the stock range of each form.

What standards does Incoloy 800 meet?

ASTM B163, ASTM B407, ASTM B408, ASME SB-407 are the standards Incoloy 800 is supplied against, each order closed by an EN 10204 3.1 mill test certificate.

When does Incoloy 800 stop being the right choice?

Incoloy 800 stops being right above 1100 °C, or in media its family was not built for.