What Incoloy 800H (N08810) can and cannot do on superalloy weldability is fixed by the verified envelope below. Datasheet facts on Incoloy 800H, and the decision they drive for superalloy weldability. Nothing else.
Incoloy 800H (N08810) is a Incoloy grade whose datasheet leans on one documented property: Enhanced creep strength vs 800.
For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.
What Superalloy Weldability means for Incoloy 800H
Incoloy 800H (N08810) on superalloy weldability: density 7.94 g/cm³, verified ceiling 1100 °C. The deciding facts are temperature, media and form, and they land on ASME pressure vessels, steam methane reformers and power plant superheaters.
| Property | Incoloy 800H |
|---|---|
| Grade | Incoloy 800H (N08810) · GB NS1102 |
| Density | 7.94 g/cm³ |
| Max service temp | 1100 °C |
| Best duty | ASME pressure vessels, steam methane reformers and power plant superheaters |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube |
| Standards | ASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII |
Specification signals
A procedure that welded the last family beautifully may be wrong for Incoloy 800H, so the grade sheet leads. In practice the applications list confirms the fit: Incoloy 800H is specified for asme pressure vessels and high-temperature heat exchangers, not as a universal filler.
- One Incoloy 800H datasheet callout does most of the work on this page: Good structural stability. A purchasing audit on the Incoloy 800H order checks that line first.
In practice
Before welding, both heats exist on certificates, and after welding the repair paperwork has to name them both again. ASME pressure vessels, steam methane reformers and power plant superheaters is practical to fabricate precisely because the weld behaviour is documented instead of guessed.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy weldability resolve for Incoloy 800H?
Welding Incoloy 800H is answered by the grade’s own procedure sheet, not by a family-wide rule. A joint is only as traceable as its paperwork. Record the heat numbers on both sides of the weld.
What is Incoloy 800H best used for?
ASME pressure vessels, steam methane reformers and power plant superheaters, which is where this grade’s datasheet numbers are actually verified.
What forms is Incoloy 800H available in?
Incoloy 800H ships as Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube, within the stock range of each form.
What standards does Incoloy 800H meet?
Every Incoloy 800H order cites its governing standard (ASTM B163, ASTM B407, ASME SB-163, ASME Section III/VIII) and arrives with an EN 10204 3.1 certificate proving the heat.
When does Incoloy 800H stop being the right choice?
Two things end it: a peak service temperature above 1100 °C, or media outside the family Incoloy 800H was built for.