A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
As strength anchors from the verified feature sets, MP35N achieves over 1800 MPa tensile while staying non-magnetic per ASTM F562, and Nimonic 80A carries gamma-prime strengthening with service to 815 °C.
What this page covers
Cobalt grades buy properties nickel cannot: ultra-high tensile, wear and galling resistance, and biocompatibility. At RAS Thermal MP35N (UNS R30035) delivers ultra-high tensile strength (over 1800 MPa achievable) and MRI-compatible non-magnetic behavior. L605 (UNS R30605) delivers wear and galling resistance with oxidation resistance to 980 °C.
The verified numbers
Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). MP35N: R30035 · >1800 MPa. L605: R30605 · 980 °C. Biocompatible: F562 · F90. Non-magnetic: both.
What this means for your selection
Cobalt grades buy properties nickel cannot: ultra-high tensile, wear and galling resistance, and biocompatibility. At RAS Thermal MP35N (UNS R30035) delivers ultra-high tensile strength (over 1800 MPa achievable) and MRI-compatible non-magnetic behavior. L605 (UNS R30605) delivers wear and galling resistance with oxidation resistance to 980 °C. The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.
How the candidate options compare
- MP35N: 8.43 g/cm³ · 425 °C, and typical use: medical implants, aerospace fasteners and high-performance springs.
- L605: 9.13 g/cm³ · 980 °C, and typical use: aerospace bearing races, wear rings and combustion hardware.