A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
As density anchors from the verified datasheets, Hastelloy X verifies 8.22 g/cm³ with oxidation resistance to 1100 °C, Inconel 625 verifies 8.44 g/cm³ to 980 °C, and L605 is the heaviest stocked grade at 9.13 g/cm³.
What this page covers
Superalloys are strengthened two ways: in solid solution, or by precipitation (aging). At RAS Thermal the precipitation-hardened grades, Inconel 718 (aged to 38 HRC), Nimonic 80A (gamma-prime), Waspaloy, gain strength from a heat treatment whose stability sets the temperature ceiling, the solid-solution grades, Inconel 625, Hastelloy C-276, Hastelloy X, Monel 400, keep strength and oxidation resistance without an aging step.
The verified numbers
Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). Precipitation-hardened: Inconel 718 / Nimonic 80A / Waspaloy / Incoloy 925. Solid-solution: Inconel 625 / Hastelloy C-276 / Hastelloy X / Monel 400 / Nickel 200 / Incoloy 800 / Incoloy 800H / Incoloy 800HT / Incoloy 825. Aged example: Inconel 718 → 38 HRC. No-aging example: Hastelloy C-276, as-welded OK.
What this means for your selection
Superalloys are strengthened two ways: in solid solution, or by precipitation (aging). At RAS Thermal the precipitation-hardened grades, Inconel 718 (aged to 38 HRC), Nimonic 80A (gamma-prime), Waspaloy, gain strength from a heat treatment whose stability sets the temperature ceiling, the solid-solution grades, Inconel 625, Hastelloy C-276, Hastelloy X, Monel 400, keep strength and oxidation resistance without an aging step. The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.
How the candidate options compare
- Inconel 718: 8.19 g/cm³ · 650 °C, and typical use: rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
- Inconel 625: 8.44 g/cm³ · 980 °C, and typical use: seawater piping, chemical processing and subsea connectors where weldability and corrosion resistance decide.
- Hastelloy C-276: 8.89 g/cm³ · 400 °C, and typical use: chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.
- Hastelloy X: 8.22 g/cm³ · 1100 °C, and typical use: gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C.
- Monel 400: 8.8 g/cm³ · 540 °C, and typical use: seawater piping, HF acid alkylation units and marine shafts.
- Nimonic 80A: 8.19 g/cm³ · 815 °C, and typical use: exhaust valves, turbine blades and high-temperature springs to 815 °C.
- Waspaloy: 8.22 g/cm³ · 870 °C, and typical use: turbine discs, rings, shafts and high-temperature fasteners.
- Nickel 200: 8.89 g/cm³ · 315 °C, and typical use: caustic soda evaporator tubes, spinnerets and electrical terminals.
- MP35N: 8.43 g/cm³ · 425 °C, and typical use: medical implants, aerospace fasteners and high-performance springs.
- L605: 9.13 g/cm³ · 980 °C, and typical use: aerospace bearing races, wear rings and combustion hardware.
- 4J29: 8.17 g/cm³ · 450 °C, and typical use: glass-to-metal and ceramic-to-metal seals in electronic packages.
- 4J36: 8.1 g/cm³ · 230 °C, and typical use: optical benches, LNG tank membranes and cryogenic transfer lines.
- 1J22: 8.2 g/cm³ · 450 °C, and typical use: solenoid armatures, pole pieces and weight-critical magnetic hardware.
- 1J50: 8.2 g/cm³ · 450 °C, and typical use: instrument transformer cores, relay armatures and shielding.
- Incoloy 800: 7.94 g/cm³ · 1100 °C, and typical use: petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.
- Incoloy 800H: 7.94 g/cm³ · 1100 °C, and typical use: ASME pressure vessels, steam methane reformers and power plant superheaters.
- Incoloy 800HT: 7.94 g/cm³ · 1100 °C, and typical use: hot-formed pressure vessel heads, tube sheets and reformer tubes.
- Incoloy 825: 8.14 g/cm³ · 540 °C, and typical use: sulfuric acid coolers, phosphoric acid evaporators and offshore production piping.
- Incoloy 925: 8.14 g/cm³ · 650 °C, and typical use: sour gas wellhead components, downhole completion tools and high-strength fasteners.
- 3J21: 8.3 g/cm³ · 350 °C, and typical use: precision instrument hairsprings, pressure sensor diaphragms and elastic sensing elements.
Related resources
Each link below takes one grade or one sub-topic and carries the same verified numbers with it.
- solution vs precipitation, Inconel 718
- solution vs precipitation, Inconel 625
- solution vs precipitation, Hastelloy C-276
- solution vs precipitation, Hastelloy X
- solution vs precipitation, Monel 400
- solution vs precipitation, Nimonic 80A
- solution vs precipitation, Waspaloy
- solution vs precipitation, Nickel 200
- solution vs precipitation, MP35N
- solution vs precipitation, L605
- solution vs precipitation, 4J29
- solution vs precipitation, 4J36
- solution vs precipitation, 1J22
- solution vs precipitation, 1J50
- solution vs precipitation, Incoloy 800
- solution vs precipitation, Incoloy 800H
- solution vs precipitation, Incoloy 800HT
- solution vs precipitation, Incoloy 825
- solution vs precipitation, Incoloy 925
- solution vs precipitation, 3J21
- Superalloy heat treatment guide (pillar)
- Waspaloy forging temperature and heat treatment
- Nimonic 80A heat treatment