The verified density of all 20 stocked grades, from Incoloy 800 at 7.94 g/cm³ to L605 at 9.13 g/cm³: with a g/cm³ · kg/m³ · lb/in³ · lb/ft³ converter.
| Alloy | Family | g/cm³ | kg/m³ |
|---|---|---|---|
| Incoloy 800 | Nickel | 7.94 | 7940 |
| Incoloy 800H | Nickel | 7.94 | 7940 |
| Incoloy 800HT | Nickel | 7.94 | 7940 |
| 4J36 | Precision | 8.10 | 8100 |
| Incoloy 825 | Nickel | 8.14 | 8140 |
| Incoloy 925 | Nickel | 8.14 | 8140 |
| 4J29 | Precision | 8.17 | 8170 |
| Inconel 718 | Nickel | 8.19 | 8190 |
| Nimonic 80A | Nickel | 8.19 | 8190 |
| 1J22 | Precision | 8.20 | 8200 |
| 1J50 | Precision | 8.20 | 8200 |
| Hastelloy X | Nickel | 8.22 | 8220 |
| Waspaloy | Nickel | 8.22 | 8220 |
| 3J21 | Precision | 8.30 | 8300 |
| MP35N | Cobalt | 8.43 | 8430 |
| Inconel 625 | Nickel | 8.44 | 8440 |
| Monel 400 | Nickel | 8.80 | 8800 |
| Hastelloy C-276 | Nickel | 8.89 | 8890 |
| Nickel 200 | Nickel | 8.89 | 8890 |
| L605 | Cobalt | 9.13 | 9130 |
Incoloy 800 at 7.94 g/cm³ (7940 kg/m³). The lightest structural nickel grades sit near 7.9-8.2 g/cm³; the heaviest stocked grade is L605 at 9.13 g/cm³.
Multiply g/cm³ by 1000 for kg/m³, and by 0.0361273 for lb/in³. For example Inconel 718 at 8.19 g/cm³ is 8190 kg/m³ and about 0.296 lb/in³. The converter above does all four units at once.
The table shows the verified datasheet figure from each grade's page on this site, the design reference. The mill certificate for your actual heat states the measured value, which can differ in the third decimal.
Send the grade, form and dimensions. We reply with the theoretical weight from the verified density and the stock range that matches.
Send your requirement