Precision alloys, the five stocked grades

The 5 precision alloys on stock, two expansion grades, two soft-magnetic grades and one high-elasticity grade, with the property each is bought for, its standards and its forms.

Grade Selected for Standards g/cm³ Max °C Forms
4J29 Expansion match to borosilicate glass ASTM F15 · GB/T 14986 · MIL-I-23011 8.17 450 Wire, Strip, Bar & Rod, Plate & Sheet
4J36 Near-zero expansion, dimensional stability ASTM F1684 · GB/T 14986 8.10 230 Wire, Strip, Bar & Rod, Plate & Sheet
1J22 Highest saturation induction (2.4 T) GB/T 14986 · ASTM A801 8.20 450 Wire, Strip, Plate & Sheet, Bar & Rod
1J50 High initial permeability, low coercivity GB/T 14986 · IEC 60404-8-6 8.20 450 Wire, Strip, Plate & Sheet, Bar & Rod
3J21 Non-magnetic high-elasticity spring alloy GB/T 14986 · YB/T 5253 8.30 350 Wire, Strip, Bar & Rod

Frequently Asked Questions (FAQ)

Why are the precision alloys grouped separately?

Because they are not bought for corrosion or creep resistance, they are bought for a physical property: a matching expansion coefficient, a near-zero expansion rate, a saturation induction, a permeability curve or an elastic modulus. Their selection logic, standards (GB/T 14986 family) and forms all differ from the nickel superalloys, which is why they get their own table.

Do the 4J and 1J numbers have international equivalents?

Yes, as property-class equivalents rather than UNS entries: 4J29 is the Kovar grade covered by ASTM F15, 4J36 is Invar 36, 1J22 is the HiperCo 50 equivalent and 1J50 the 50% Ni-Fe soft magnetic grade. The equivalent-grades tool shows the full designation cross-reference for the stocked grades.

Which precision alloy is non-magnetic?

3J21, the Co-Ni-Cr-Mo high-elasticity alloy keeps non-magnetic behaviour with long-term dimensional stability, which is why it appears in instrument springs. The two 1J grades are the opposite: they are selected precisely because they are strongly magnetic.

Buying for a physical property?

Send the property target, expansion coefficient, permeability, modulus, and the form. We confirm which stocked grade meets it and quote with the certificate to prove it.

Send your requirement
Request a Quote
Add RAS Thermal as a preferred source on Google