Reference table

Governing standards by alloy

The verified ASTM, AMS, ASME, NACE and GB standards behind every stocked grade: the documents a certificate should cite. Filter by standard family or search by grade.

Inconel 718

AMS 5662AMSAMS 5663AMSASTM B637ASTM/ASMEUNS N07718GB / national

Inconel 625

ASTM B443ASTM/ASMEASTM B444ASTM/ASMEASTM B446ASTM/ASMEAMS 5666AMSNACE MR0175NACE sour

Hastelloy C-276

ASTM B575ASTM/ASMEASTM B574ASTM/ASMEASTM B564ASTM/ASMEUNS N10276GB / national

Hastelloy X

AMS 5536AMSAMS 5754AMSASTM B435ASTM/ASMEASTM B572ASTM/ASME

Monel 400

ASTM B164ASTM/ASMEASTM B127ASTM/ASMEASTM B165ASTM/ASMENACE MR0175NACE sour

Nimonic 80A

ASTM B637ASTM/ASMEBS HR 201GB / nationalAMS 5763AMSDIN 17742GB / national

Waspaloy

AMS 5708AMSAMS 5709AMSAMS 5544AMSASTM B637ASTM/ASME

Nickel 200

ASTM B160ASTM/ASMEASTM B161ASTM/ASMEASTM B162ASTM/ASMEASME SB-160ASTM/ASME

MP35N

ASTM F562ASTM/ASMEAMS 5844AMSAMS 5845AMSISO 5832-6GB / national

L605

AMS 5759AMSAMS 5537AMSASTM F90ASTM/ASME

4J29

ASTM F15ASTM/ASMEGB/T 14986GB / nationalMIL-I-23011GB / national

4J36

ASTM F1684ASTM/ASMEGB/T 14986GB / nationalAFNOR NF A54-301GB / national

1J22

GB/T 14986GB / nationalAMS 7717 equivalentAMSASTM A801ASTM/ASME

1J50

GB/T 14986GB / nationalIEC 60404-8-6GB / national

Incoloy 800

ASTM B163ASTM/ASMEASTM B407ASTM/ASMEASTM B408ASTM/ASMEASME SB-407ASTM/ASME

Incoloy 800H

ASTM B163ASTM/ASMEASTM B407ASTM/ASMEASME SB-163ASTM/ASMEASME Section III/VIIIASTM/ASME

Incoloy 800HT

ASTM B163ASTM/ASMEASTM B407ASTM/ASMEASME SB-163ASTM/ASMENACE MR0175NACE sour

Incoloy 825

ASTM B163ASTM/ASMEASTM B423ASTM/ASMEASTM B424ASTM/ASMENACE MR0175NACE sour

Incoloy 925

ASTM B805ASTM/ASMENACE MR0175NACE sourAPI 6AGB / national

3J21

GB/T 14986GB / nationalYB/T 5253GB / national

Frequently Asked Questions (FAQ)

What does the governing standard decide?

It is the document the mill certificate is written against: chemistry window, condition, test methods and sizes all come from it. Two grades with near-identical chemistry can be non-conforming to each other's document, so the standard belongs on the drawing, not assumed from the grade name.

Why do some grades list AMS numbers?

AMS (SAE aerospace material specifications) add controlled melt practice, tighter trace-element limits and, for some numbers, a delivered heat-treatment condition. Grades stocked for aerospace duty carry both their ASTM baseline and the AMS documents where they apply.

What does NACE MR0175 on a grade mean?

It is the sour-service qualification layer, hardness and chemistry limits for H₂S exposure, on top of the mill grade. It is a service qualification, not a grade change; the certification page goes deeper on what the certificate must then prove.

Matching the standard to the form?

Send the duty and the form, we confirm the governing document pair (plate, bar, tube, forging) and quote against it with a heat-traceable certificate.

Send your requirement
Request a Quote
Add RAS Thermal as a preferred source on Google