Forged Alloy Components
Open-die, ring-rolled or upset: nickel, cobalt and precision alloy forgings from 5 kg to 3,000 kg.
Forging Capabilities
§01, OverviewRAS Thermal forges rings, discs, shafts, blocks and custom shapes in heat-resistant and corrosion-resistant alloys. Upsetting, ring-rolling, open-die and closed-die all run in-house, with heat treatment and NDT on the same floor. One heat number follows the part from billet to certificate.
Key Capabilities
- Weight range
- 5 kg - 3,000 kg
- Ring OD
- Up to 2,500 mm
- Max length
- Up to 6,000 mm
- Heat treatment
- Solution + age, anneal, stress-relief
- NDT
- UT, MT, PT, dimensional CMM
Why RAS Thermal
§02, Quality + TraceabilitySizes & Tolerances
§03, Specifications| Type | Range | Note |
|---|---|---|
| Rings | OD 100 - 2,500 mm | Wall 15 - 400 mm |
| Discs | Ø 100 - 1,200 mm | Thickness 30 - 600 mm |
| Shafts | Ø 50 - 500 mm | Length up to 6,000 mm |
| Custom blocks | By drawing | 5 kg - 3,000 kg |
Tolerances
- Dimensional
- ASTM B564 / customer PO
- Surface finish
- Ra 6.3 - 25 as forged
- Machined finish
- Ra 0.8 - 3.2 on request
Typical End Uses
§04, ApplicationsFrequently Asked Questions
Forging FAQWhat forging sizes can you produce in Inconel 718 and other nickel alloys?
From 5 kg to 3,000 kg depending on process. Ring-rolled parts reach 2,500 mm OD with 15-400 mm wall, discs go to Ø1,200 mm, shafts to Ø500 mm × 6,000 mm long. Heat treatment (solution + age or annealed), UT/MT/PT inspection and a furnace-batch-traceable MTC come with every delivery.
Which standards govern your nickel alloy forgings and flanges?
ASTM B564 and ASME B16.5 govern the forgings. Age-hardened grades carry AMS 5662 for Inconel 718 and AMS 5708 for Waspaloy, sour-service items add NACE MR0175 qualification, and flanges ship with PMI report plus hydrostatic test documents when the PO asks for them.
Can you supply machined forgings for subsea and downhole service?
Yes. Rough or finish-machined blocks, wellhead connectors and pump shafts in Inconel 718, 625 and Monel K-500 all ship to NACE MR0175 hardness limits, CMM dimensional report included, each piece traceable to its heat.