A hermetic package is not one that is filled with an inert gas, it is one whose leak rate has been measured against a number on the drawing. For 4J29 (Kovar) that number is the site-verified 10⁻⁹ cc He/s acceptance figure, and it only means something together with the helium fine-leak test method and the seal partner it was proven against. This guide covers the criterion, the partners the expansion match actually covers, the form each package family uses, and the failure modes to design out.

What “hermetic” means in numbers

Hermeticity is a leak-rate specification, not a label. The verified acceptance figure for 4J29 on this site is 10⁻⁹ cc He/s, measured by a helium fine-leak test: the package is pressurised with helium, then the helium escaping the sealed volume is measured on a mass spectrometer. Two things belong on the drawing whenever that figure is quoted, because they change what is being promised:

  1. The criterion, written as a number and a unit (10⁻⁹ cc He/s), not as the word “hermetic”.
  2. The test method and sequence: a fine-leak helium test after the sealing step, and whether a gross-leak screen precedes it.

Without both, “hermetic” drifts into a marketing word, and two suppliers can accept the same drawing while testing to different criteria.

The expansion match is a property of the pair

4J29 exists for one property: its thermal expansion matches borosilicate glass and alumina ceramics closely enough for a sealed joint to survive the cooling from sealing temperature to service without the metal yielding or the glass cracking. That match is a property of the pair, not of the alloy alone. Two consequences follow. First, the seal partner has to be named on the drawing, a different glass family, or a hard-soldered rather than a glass-sealed joint, changes the stress state and voids the match the datasheet covers. Second, if the partner changes, the match has to be re-proven, the alloy is rarely the variable when a package leaks.

Form follows the package family

The stocked forms, Wire, Strip, Bar & Rod, Plate & Sheet, map onto the listed applications directly:

Package familyTypical formSeal partner
Transistor and IC hermetic packagesStrip, plate & sheetBorosilicate glass
Microwave tube windowsPlate & sheetGlass / alumina ceramic
Optoelectronic device housingsPlate & sheetBorosilicate glass
Reed switch glass sealsStripBorosilicate glass
Cryogenic electrical feedthroughsWireGlass / alumina ceramic

Strip carries the pressed lead frames and reed blades, wire carries matched-diameter feedthrough pins, plate and sheet carry the package headers and tube windows. The form is a consequence of the seal geometry, so choose the geometry first and let it pick the form.

Where a hermetic seal actually fails

When a sealed package leaks, the path is almost always at the interface, not through the metal. The four recurring causes are worth designing out rather than testing for:

  • Partner mismatch: the alloy and the glass riding different expansion curves, so the interface is stressed on every thermal cycle.
  • Surface state at the seal: oxide condition and plating control how the glass wets and bonds, a good alloy with the wrong surface still leaks.
  • Thermal cycling: each cycle works the interface, a joint that passes a one-off test can still fail after thermal fatigue.
  • Process choice: glass sealing versus hard soldering imposes a different temperature and stress history on the same alloy, and one cannot be substituted for the other without re-verifying hermeticity.

All four are process-and-design questions, which is why hermeticity is specified as a measured criterion and a named partner rather than inferred from the alloy grade.

How to specify a hermetic 4J29 part

Write the requirement so the seal can be audited:

  • Grade and standard: 4J29 (Kovar) against ASTM F15 / GB/T 14986 / MIL-I-23011.
  • Leak criterion and method: the 10⁻⁹ cc He/s fine-leak figure with the helium test method and sequence.
  • Seal partner: the specific glass or ceramic, named, not “glass-to-metal” as a category.
  • Service envelope: the verified ceiling is 450 °C; above it the datasheet guarantee ends.
  • Certificate: EN 10204 3.1 chemistry against the cited standard, plus the leak-test record for the production lots.

The RFQ spec writer assembles the enquiry, the 4J29 vs 4J36 comparison separates the expansion-match grade from the near-zero-expansion grade, which are often confused but do different jobs.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

What leak rate makes a 4J29 package hermetic?

The verified acceptance figure on this site is 10⁻⁹ cc He/s, measured by a helium fine-leak test. Hermeticity is a measured criterion, so the number and the test method both belong on the drawing, “hermetic” without them is not testable.

Can 4J29 seal against any glass?

No. The verified expansion match is specifically to borosilicate glass and alumina ceramics. A different glass family, or a hard-soldered joint instead of a glass seal, changes the stress state at the interface and the match has to be re-proven.

Why does a hermetic 4J29 package leak if the alloy expansion matches the glass?

Because the match is a property of the pair, not of the metal. Leak paths usually appear at the interface, from partner mismatch, the oxide and plating state at the seal, thermal fatigue, or a change between glass sealing and hard soldering. The alloy is rarely the variable when a package leaks.

What is the maximum service temperature for a 4J29 seal?

The verified ceiling is 450 °C. Above it the datasheet guarantee ends, and the expansion match the seal was designed around is no longer covered by the grade’s own documentation, the seal has to be re-qualified for the higher temperature rather than assumed to hold.