Hastelloy C-276 is designated UNS N10276 in the US, W.Nr 2.4819 (EN NiMo16Cr15W) in Europe, NW 0276 in Japan, ХН65МВУ / ЭП760 in the GOST system and NS334 in China. As with all nickel alloys, the more useful cross-reference is not the grade name but the form standard: ASTM B575 for plate, sheet and strip, B574 for bar, B622 for seamless tube and B564 for forgings. State the form-standard pairing and the certificate level, the national designation alone does not define the acceptance.
Hastelloy C-276 equivalent standards at a glance
| System | Designation |
|---|---|
| USA (UNS) | N10276 |
| Germany (W.Nr.) | 2.4819 |
| EN | NiMo16Cr15W |
| Japan | NW 0276 |
| Russia (GOST) | ХН65МВУ · ЭП760 |
| China | NS334 |
NACE MR0175 / ISO 15156 applies on top wherever the component sits in sour (H₂S) service: it is a service qualification, not a mill grade.
The ASTM standard that owns each form
| Product form | Governing ASTM standard |
|---|---|
| Plate, sheet, strip | ASTM B575 |
| Rod and bar | ASTM B574 |
| Seamless pipe and tube | ASTM B622 |
| Welded pipe and tube | ASTM B619 / B626 |
| Forgings | ASTM B564 |
| Pipe fittings | ASTM B366 |
This is the matrix that matters at purchase: a C-276 plate certified to B575 is not interchangeable with a bar certified to B574 on the paper trail, even though the chemistry is the same. Cite the form standard your drawing requires.
The chemistry that defines the grade
Verified composition windows for C-276 as supplied on this site:
| Element | Range | Role |
|---|---|---|
| Ni | Balance | Matrix |
| Mo | 15.0-17.0 % | The principal corrosion driver |
| Cr | 14.5-16.5 % | Oxidising-media resistance |
| Fe | 4.0-7.0 % | Matrix balance |
| W | 3.0-4.5 % | Reinforces the Mo effect |
| Co | ≤ 2.5 % | Residual |
| C | ≤ 0.01 % | Low-carbon to protect weld-zone corrosion resistance |
The molybdenum and tungsten content, and the low carbon limit, are what make C-276 resistant to pitting, crevice and stress-corrosion cracking across a wide acid range, and weldable without post-weld heat treatment. Its verified room-temperature mechanicals are 790 MPa UTS / 355 MPa yield / 40%, with service to 400 °C and density 8.89 g/cm³.
Why C-276 and C-22 are not interchangeable
Both are Ni-Cr-Mo alloys, but they are not the same grade, and the ASTM B575 chemistry windows separate them on chromium and molybdenum, not on tungsten. C-276 carries 14.5-16.5 % Cr with 15.0-17.0 % Mo; C-22 carries 20.0-22.5 % Cr with 12.5-14.5 % Mo; each also contains tungsten (3.0-4.5 % in C-276, 2.5-3.5 % in C-22). C-276’s higher molybdenum is the reference for reducing acids. C-22’s higher chromium gives it the edge in oxidising and mixed-acid service. Because the two look identical on a finished part, the practical safeguard is verification rather than paperwork alone: full OES analysis reconciled line by line to the marked heat number and the EN 10204 3.1 certificate. Handheld XRF cannot separate the grades reliably, because the discriminator is a chromium-versus-molybdenum ratio rather than the presence of one element, insist on OES or spark analysis.
How to specify C-276
Name the grade and UNS (Hastelloy C-276, UNS N10276), the form and its standard (B575 plate, B574 bar, B622 seamless tube, B564 forging), the condition (solution annealed) and the certificate (EN 10204 3.1 heat chemistry, or 3.2 witnessed for project work). Add NACE MR0175 / ISO 15156 where the duty is sour. A validity-dated quote against that specification is the only price that holds, see the C-276 price per thickness and C-276 plate weight and price pages for the indicative bands.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
What is the European equivalent of Hastelloy C-276?
W.Nr 2.4819 / EN NiMo16Cr15W. In Japan it is JIS NW 0276, in Russia GOST ХН65МВУ (ЭП760), and in China NS334. All refer to UNS N10276.
Which ASTM standard covers C-276 plate?
ASTM B575 covers low-carbon Ni-Cr-Mo plate, sheet and strip. Bar is B574, seamless tube is B622, and forgings are B564, cite the form standard on the purchase order.
Is C-276 the same as C-22?
No. C-276 (UNS N10276) carries 15-17 % molybdenum plus 3-4.5 % tungsten and is the reference for reducing acids and wet chlorine; C-22 (N06022) has higher chromium for broader mixed-acid tolerance. They are different grades and must not be substituted without engineering review.
How do I verify a C-276 heat?
By full OES or spark analysis reconciled line by line against the marked heat number and the EN 10204 3.1 certificate. Both C-276 and C-22 contain tungsten, so the discriminator is the chromium and molybdenum ratio, C-276 at 14.5-16.5 % Cr with 15.0-17.0 % Mo against C-22 at 20.0-22.5 % Cr with 12.5-14.5 % Mo, not the presence of a single element. Handheld XRF is not reliable enough for that distinction.