Inconel 718 is one of the few grades where the delivery condition can change the invoice more than the alloy itself. The metal is the same in all four states; what differs is how many process steps have already been run before the material reaches you, and who carries the yield loss. This page sets out those states in cost order, gives the exact weight arithmetic, and points at the page that prices the grade itself.
The per-kilogram number is deliberately not published here. The alloy charge re-prices with the nickel index and the ageing cost depends on lot size, so a printed band would be wrong before it shipped — the reasons are set out on the Inconel 718 price page, which also gives the verifiable nickel floor.
The four states, in cost order
| Delivery condition | Position | What has been done to it | What you still carry |
|---|---|---|---|
| Black / hot-rolled bar | Entry | Rolled and cooled only | Machining, heat treatment, distortion, scrap |
| Peeled / ground, solution annealed | Mid | Surface removed to a controlled diameter, then annealed | Machining; ageing still to be done |
| Solution treated, then aged | Upper mid | Solution anneal plus two-step age, tested per lot | Machining of harder material |
| Solution + aged to AMS 5662 | Top | As above plus the rotating-quality inspection package | Nothing beyond final machining |
Read that table as a ranking of process steps, not of metal. Two enquiries for the same tonnage can differ substantially with neither supplier being wrong — one is quoting black bar, the other AMS-grade aged bar with third-party documentation.
What each step actually costs you
Black bar. You buy the alloy and the rolling. Everything downstream — the saw, the lathe, the furnace — is yours, and so is the swarf and the scrapped pieces. On a part with heavy stock removal this is usually the cheapest route, and on a near-net part it is usually not.
Peeling and grinding. Removing the surface to a controlled diameter adds machining time and converts a fraction of the bar into chips. That fraction is bought at alloy price and recovered, if at all, at scrap price — which is why the step costs more than the machining hours suggest, particularly on small diameters where the surface layer is a bigger proportion of the section.
Solution plus ageing. Two furnace cycles with holds measured in hours, plus hardness and tensile testing per lot. The properties depend on the cycle, not on the chemistry, so every lot has to be proven rather than assumed. This is the step that puts 718 above 625 on cost despite 718 containing less nickel — a comparison worked through on the 718 price page.
AMS 5662 package. Where rotating quality applies, the inspection and documentation requirements attach to the ageing step and cannot be separated from it. They add time and cost even though the alloy has not changed.
Worked example: weight, done correctly
A Ø50 mm × 3,000 mm bar of Inconel 718, at the verified density of 8.19 g/cm³:
- Cross-section: π × (25 mm)² = 1,963.5 mm²
- Per metre: 1,963.5 mm² × 1,000 mm = 1,963,500 mm³ = 1,963.5 cm³
- Unit weight: 1,963.5 cm³ × 8.19 g/cm³ = 16.08 kg per metre
- Piece weight (3 m): 48.2 kg
That figure is exact and checkable. What you then multiply it by is a price your supplier has to quote, for a stated condition, standard and quantity — and it is worth noting that a bar this size is comfortably a mill product, so it does not carry the small-lot surcharge that a 50 kg order in an unusual section would.
Use the weight calculator by grade and form for other geometries, and the six costing mistakes page before you set a budget — input mass versus finished mass is the single most common overrun on this grade.
How to get a firm quote by condition
A quote is valid only against a defined specification. Send:
- Grade and UNS (N07718)
- Form, dimensions and quantity with unit
- Condition — black, peeled, solution annealed, aged, or aged to AMS 5662
- Governing standard — ASTM B637 for bar and forging stock, AMS 5662 where rotating quality applies
- Certificate level — EN 10204 3.1 with heat-specific chemistry, or 3.2 witnessed
- Incoterm and destination port
The RFQ spec writer assembles those lines. Two quotes that both state condition and certificate level can be compared; two that state only a grade cannot.
Why condition is the first question, not the last
Buyers usually start with the grade and the price, and discover the condition question when the first lot fails inspection or when the machined part distorts in the furnace. Starting with the condition reverses that: it fixes how much process is being bought, which fixes the yield, which is what the invoice is actually made of. The grade then sets the alloy floor on top.
Frequently Asked Questions (FAQ)
Which delivery condition of Inconel 718 is cheapest?
Black hot-rolled bar. No finishing and no ageing have been applied, so you pay for the alloy and the rolling only. The catch is that you then machine and heat-treat it yourself, and you absorb the distortion and the scrap that come with that.
How much does peeling and grinding add?
It removes surface defects and brings the bar to a controlled diameter, which adds machining time and turns part of the bar into swarf bought at alloy price and sold at scrap price. On small diameters that yield loss is a larger share of the cost than the machining time.
Why is solution plus aged material the most expensive condition?
Two furnace cycles — solution treatment and a two-step age — plus mechanical testing per lot, because the properties come from the cycle and not from the chemistry alone. Where AMS 5662 applies for rotating quality, the inspection and documentation package sits on top of that.
Does 718 need ageing if I machine it from black bar?
If the part needs the strength 718 is bought for, yes. Machining in the solution-treated condition is easier on tooling and the part is aged afterwards, which means accepting distortion in heat treatment. Buying aged bar and machining it means harder cutting but no post-machining heat treatment.
How do I turn a drawing into a budget?
Compute the exact weight from density × volume, add the input-mass allowance for your process, then apply the price your supplier quotes for that grade, form, condition and quantity. The weight is exact and repeatable; the price is not, because it moves with the nickel index and with your lot size.
Why does this page not state a price per kilogram?
Because the alloy charge re-prices with the nickel index and the ageing cost depends on lot size, so a printed band is stale before it ships. The ordering between conditions is stable and is published here; the number comes from a validity-dated quote against a defined specification.