Six Costing Mistakes
Almost every nickel alloy budget overrun is arithmetic, not market movement. Six calculations, in the order they go wrong.
The metal did not get more expensive
§01, Why budgets breakWhen a nickel alloy job comes in 30–40% over budget, the instinct is to blame the alloy market. Usually it is not. It is the difference between the mass the drawing describes and the mass the invoice is based on, plus a handful of process assumptions that were never priced.
Each of the six below is checkable before a purchase order exists. Each has a specific number attached, and the fix is a sentence in the enquiry rather than a negotiation.
Density, from the specification
| Grade | UNS | g/cm³ |
|---|---|---|
| GH3044 | N06604 | 8.89 |
| Inconel 625 | N06625 | 8.44 |
| Hastelloy X | N06002 | 8.22 |
| Inconel 718 | N07718 | 8.19 |
| Incoloy 800H | N08810 | 7.94 |
Source: the grade specifications cited on each datasheet. Mild steel is 7.85 g/cm³ — using it for GH3044 understates mass by 13%.
01
Costing by density alone, and using the wrong density
- What happens
- Nickel alloy is bought by weight, so the whole budget rests on one number: density. Use the alloy's own value, not 7.85 g/cm³ from mild steel.
- What it costs
- GH3044 at 8.89 g/cm³ is 13% heavier than 800H at 7.94 for the same drawing. On a furnace order sized on steel density, that is a 13% budget overrun before anyone quotes anything.
- The fix
- Take density from the grade specification, and run the arithmetic on net finished mass. The weight calculator on this site uses the specification values for each grade.
02
Budgeting net weight while the mill charges gross
- What happens
- A drawing gives finished dimensions. A mill quote covers the input mass: cut allowance, machining stock, end trim and the piece you lose to the saw.
- What it costs
- On a 20 mm bar turned down to 15 mm, roughly 44% of the input volume becomes swarf — and swarf is bought at alloy price and sold at scrap price.
- The fix
- Multiply net mass by a realistic yield factor for the process before you compare with a quote. Ask the supplier what input mass their price is based on; it is the single question that closes most of the gap.
03
Comparing per-piece prices across different input masses
- What happens
- Two suppliers quoting 'the same part' per piece may be working from different stock sizes and therefore different input mass.
- What it costs
- A part cut from 25 mm bar and the same part cut from 30 mm bar can show a 15–20% price difference with identical finished dimensions and identical alloy.
- The fix
- Ask each quote to state stock size and input weight per piece. Compare cost per kilogram of input, not cost per piece.
04
Treating tolerance class as free
- What happens
- Commercial tolerance is what a mill produces by default. A drawing with a tight flatness, concentricity or thickness tolerance is a different process.
- What it costs
- Straightening, additional passes, extra inspection and higher scrap all attach to the tighter tolerance. On thin sheet the difference between commercial and precision can be the largest single line in the quote.
- The fix
- Mark which tolerances are functional and which are drafting habit. Relaxing one non-functional callout often removes an entire process step.
05
Comparing FOB with CIF, and forgetting duty
- What happens
- FOB ends at the export port. CIF adds freight and insurance. DAP adds delivery. Import duty and clearance sit outside all three.
- What it costs
- On heavy alloy shipments freight is a modest share, but on small parcels and air shipments it can exceed the metal cost difference between two suppliers.
- The fix
- Convert every quote to a landed cost at your own door, in your own currency, including duty. Then compare. A supplier can be cheapest FOB and dearest landed.
06
Assuming a grade substitution is cost-neutral
- What happens
- Buyers sometimes swap a grade late in a project to relieve a delivery problem, expecting the budget to hold.
- What it costs
- Density, machinability, welding procedure, heat treatment and certificate basis all change with the grade. 625 to 718 adds an ageing cycle; 718 to 625 loses strength and may force a section change; GH3044 to Hastelloy X changes the certificate standard entirely.
- The fix
- Treat a grade change as a re-quote, not a substitution. Ask for the delta in input mass, process steps and test scope — all three move, usually in the same direction.
One plate, two budgets
§03, Worked exampleA 100 × 100 × 10 mm plate in Inconel 625, finished mass 84.4 g. Watch where the two budgets diverge before anyone negotiates a price.
| Line | Drafting-habit budget | Cost-engineered budget |
|---|---|---|
| Density used | 7.85 g/cm³ (steel) | 8.44 g/cm³ (625) |
| Mass costed | 78.5 g | 84.4 g net |
| Input mass for the process | 78.5 g assumed | Stock allowance added, then yield applied |
| Tolerance class priced | Not stated | As-drawn quoted separately |
| Delivery basis | FOB | Landed, including duty |
The column on the left is not a wrong price. It is a price for a different object: a steel-density, commercial-tolerance, FOB article. The gap to the right-hand column is what shows up as an overrun later.
Eight questions, answered
§04, QuestionsHow much does a 10 mm thick, 100 × 100 mm plate weigh in each grade?
The volume is 100 cm³. At specification density that gives 889 g in GH3044 (8.89 g/cm³), 844 g in Inconel 625 (8.44), 822 g in Hastelloy X (8.22), 819 g in Inconel 718 (8.19) and 794 g in Incoloy 800H (7.94). Those are net figures — the mill will charge for the input mass, which is larger.
What yield factor should I assume when budgeting a machined nickel alloy part?
It depends on how much material the process removes. A part near-net-forged may run at 85–90% yield; a part turned from bar down to half its diameter can lose more than half the input mass. Rather than assume a number, calculate: input mass ÷ finished mass is your real multiplier, and it is the figure to apply to the per-kilogram price before you compare with a budget.
Why is swarf not credited back at the metal price?
Because turning alloy bar into chips destroys the form the mill sold you, and recovery is a separate melting route with its own cost and its own market. Expect scrap credit to be a fraction of the purchase price, and expect it to be quoted separately, if at all. Budget the full input mass as cost and treat any scrap credit as upside.
Does a tighter tolerance really change the price that much?
It changes the number of process steps, and steps cost more than metal on small parts. Straightening, extra grinding passes, dimensional inspection and the yield loss from rejected pieces all attach to the tighter callout. The way to find out is to ask for two prices on the same part — commercial and as-drawn — and see the delta on your specific geometry.
Is it cheaper to buy a heavier standard size and machine down?
Often yes, and it is worth asking. Standard mill sizes are produced in volume and priced accordingly; a bespoke size carries a setup share. The comparison is straightforward once you have both input masses: cost per kilogram × input mass, plus machining time. Buying heavier stock to save a setup is a common and legitimate saving.
How do I compare a Chinese FOB quote with a European delivered quote fairly?
Convert both to landed cost at your own facility: add freight, insurance, duty, clearance and any inspection you require, then convert to one currency at the same date. Only then compare. Also normalise the certificate level and test scope, because a European price that includes third-party inspection and a Chinese price that excludes it are not the same product.
What is the single most common costing error on nickel alloy jobs?
Budgeting from finished weight. The drawing gives the finished part; the invoice is based on input mass plus process. Every downstream surprise — yield loss, remelt policy, tolerance class — is a consequence of that first assumption. Fix the input-mass calculation and most of the overrun disappears before it happens.
Can you quote on both net weight and input weight so I can see the difference?
Yes, and for repeat parts it is worth asking for. A quote that states the input mass per piece alongside the price lets you compare suppliers on the same basis and lets you see immediately whether a cheaper quote is cheaper metal or lighter input.
Where these numbers come from
§05, NextSend the drawing, get input mass and price together
Ask for a quote that states stock size, input mass per piece and the tolerance class priced. Then the comparison with your budget is arithmetic instead of a surprise.
Request a costed quote