Inconel 625 forged bar and plate at the RAS Thermal works
Cost Guide / Inconel 625

Inconel 625 Price

What sits behind the price of one kilogram in 2026, which six variables move the number, and how to compare two quotes that were never written on the same basis.

The short answer

§01, Summary

Published price

No fixed band — priced per enquiry

The metal moves with the nickel index weekly, and the answer depends on form, size, melting route and test scope. A number printed here would be wrong before the next shipment.

Nickel floor today

USD 8.88/kg

58% nickel × LME cash of USD 15,310/t on 2026-11-20. This is the nickel content only — before Cr, Mo, Nb, melting and rolling.

What changes it most

Form → size → melting route → test scope

Two quotes for the same tonnage can differ by 40% without either being wrong, if one is ESR plate and the other is VAR bar with 100% UT.

Cost position by product form

§02, Where each form sits

We do not publish per-kilogram bands: the alloy charge re-prices with nickel and molybdenum, so any figure here would be out of date before it shipped. What does not change is the relative position of each form — that is what decides which enquiry costs more, and it stays true whatever the index does.

Product form Standard Cost position Why it sits there
Hot-rolled plate, 3–25 mm ASTM B443 Lowest Standard mill route; the shortest conversion path from melt to product
Hot-rolled round bar, 20–60 mm ASTM B446 Low to mid Catalogue sizes are routine; peeling and straightening add steps
Cold-rolled sheet, 0.5–3 mm ASTM B443 Mid Cold reduction, annealing and pickling passes, plus finish control
Forged bar, 60–200 mm ASTM B446 Mid to high Press capacity, press time and a higher inspection burden
Seamless pipe ASTM B444 Highest Piercing and cold drawing; the longest and least forgiving route

Read it as a ranking, not as a price list. Two enquiries for the same form can still differ by a third — see the six variables in section 04 — but plate will not overtake pipe because nickel moved.

How one kilogram is priced

§03, Cost build-up

625 is not priced by the tonne like rebar. It is priced from chemistry upward, then loaded with conversion cost. Every element below is quoted to a range in ASTM B443/B444/B446, so the alloy charge is computed against the certified heat analysis, not against a nominal figure.

Element wt % Role in the cost
Nickel58.0 minDominant line; indexed to LME
Chromium20.0–23.0Ferrochrome, moderate volatility
Molybdenum8.0–10.0Second-largest; wide swings
Niobium + Tantalum3.15–4.15Small mass, high unit cost
Iron5.0 maxResidual; negligible

Composition basis: ASTM B443 / B444 / B446 (UNS N06625). GB/T equivalent: GH3625.

Worked example — the nickel line

LME nickel cash, 2026-11-20
USD 15,310/t
Per kilogram of nickel
USD 15.31
Nickel in 1 kg of 625 (58%)
USD 8.88
Sensitivity
USD 0.58 per USD 1,000/t

Add chromium, molybdenum, niobium and tantalum, then melting, rolling or forging, heat treatment, testing and yield loss. The finished band in section 02 is what that stack looks like after a mill has done it a few thousand times.

Source: LME official cash settlement via Westmetall. Verify the current figure.

Six things that move the number

§04, Variables
01

Product form

Plate and bar come off standard mill routes. Seamless pipe needs piercing and cold drawing, which is why the same alloy charges roughly double per kilogram.

02

Size and tolerance

A commercial-tolerance 40 mm bar is a catalogue item. A 0.1 mm concentricity ring is a forging plus machining job, and machining hours are not alloy-priced.

03

Melting route

Air-melted or ESR material to ASTM covers most chemical duty. VAR under AMS 5666 for aerospace and nuclear adds conversion cost and a longer route.

04

Order quantity

A single heat has a minimum economic size. Small lots carry part of that heat's fixed cost, which is why 200 kg can cost more per kilogram than 2 tonnes.

05

Test scope

Chemistry plus tensile is standard. Add ultrasonic inspection, hardness verification for NACE MR0175, or a third-party witness and you have added days and cost, not a discount.

06

Documentation level

An EN 10204 3.1 certificate tied to the heat number is normal for this alloy. If a quote does not state the certificate type, that is the first thing to ask about, not the last.

Normalise before you compare

§05, Comparing quotes

Most "625 is cheaper here" conclusions are an artefact of two quotes written on different bases. Put both on the same row before you decide.

Item to normalise What to ask Why it changes the number
IncotermFOB, CIF or DAP?Freight and insurance either are or are not in the figure
Melting routeAir / ESR / VAR?Cleanliness and conversion cost differ materially
CertificateEN 10204 3.1 to the heat?Traceability paperwork has a real cost
ToleranceCommercial or drawing?Machining and scrap are charged at alloy price
Test scopeUT, PMI, hardness, third party?Each adds a step and a schedule slot
ValidityHow long is the price held?Nominal alloy prices move weekly; a long window is a risk loaded elsewhere

625 against the grades it competes with

§06, Alternatives

Unit cost is shown as a multiple of 316L rather than in dollars, because that ratio holds across markets and currencies better than any single figure.

Grade UNS Cost vs 316L Max temp Seawater Choose it when
316L S31603 1× 400 °C No No chlorides, low temperature, budget-first
Incoloy 825 N08825 1.5–2× 540 °C Limited Sulphuric/phosphoric acid, moderate chlorides
Inconel 625 N06625 3–4× 980 °C Yes Seawater + high temperature + welds without PWHT
Hastelloy C-276 N10276 4–6× 1040 °C Yes Wet chlorine, hypochlorite, severe reducing acids
Inconel 718 N07718 4–5× 650 °C (aged) Limited Strength at temperature matters more than corrosion

When 625 is over-specified

§07, Honest advice

Below 400 °C, no chlorides

316L or 304L does the job at roughly a quarter of the metal cost. We will say so rather than quote you 625.

Sulphuric or phosphoric acid, moderate temperature

Incoloy 825 is usually adequate and materially cheaper. 625 becomes the right answer once chlorides enter the duty.

Strength, not corrosion, is the driver

If you need strength to 650 °C with aging, 718 is the better route. If you need to 980 °C without PWHT, that is exactly where 625 earns the premium.

Six ways buyers overpay

§08, Buying mistakes
01

Specifying VAR by default. VAR is for aerospace and nuclear. On chemical plant it buys certification you may not need.

02

Buying to drawing when a mill form would do. A 200 mm bar cut from a forged bloom often replaces a bespoke forging at half the process cost.

03

Splitting a heat across two suppliers. Two small lots each carry a heat's fixed cost; one consolidated lot usually costs less in total.

04

Not stating the certificate level. EN 10204 3.1 to the heat is the norm for 625. Discovering that after delivery costs more than specifying it up front.

05

Comparing a CIF price with an FOB price. Normalise the Incoterm before concluding anything about the metal cost.

06

Ignoring niobium in the chemistry check. Nb+Ta is 3.15–4.15%. Material at the bottom of that range is cheaper to make and weaker in service; check the certified analysis.

What to send for a firm quote

§09, Enquiry

Send these seven items and the first reply can be a price rather than a question.

▸

Product form — plate, sheet, bar, forging, wire, flange or pipe

▸

Size, or a drawing if the part is not a mill form

▸

Quantity with unit — pieces, kilograms or metres

▸

Governing standard — ASTM B443 / B444 / B446, AMS 5666 or GB/T GH3625

▸

Test scope and certificate level — EN 10204 3.1, UT, PMI, NACE MR0175

▸

Incoterm and destination port

▸

Required date, and whether partial shipments are acceptable

Lead time, packing and documents

§10, Delivery

Lead time

Depends on whether the item is cut from stock or rolled to order, and on the test scope. It is stated as a dated commitment on the quotation, not as a generic promise.

Packing

Bar and plate ship on timber, interleaved and edge-protected; wire ships on spools or in coils. Sea-worthy export packing is confirmed per order against the route.

Documents

Mill test certificate to EN 10204 3.1 with heat number, packing list, invoice, and certificate of origin where the destination requires it. Third-party inspection can be arranged.

Ten questions buyers ask before ordering

§11, Procurement questions

These are the questions that come up in almost every 625 enquiry. The answers are the same ones our sales engineers give on the phone.

How much does Inconel 625 cost per kg?

We quote per enquiry rather than publishing a band, because the alloy charge moves with nickel and molybdenum and any printed figure would age badly. What can be stated precisely is the metal floor: at 58% nickel and an LME cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of 625 is about USD 8.88 — before chromium, molybdenum, niobium, melting, rolling and testing. Everything above that floor depends on form, size, melting route, test scope and quantity. Send those and you get a number valid for a stated period.

Why is the price of Inconel 625 so much higher than stainless steel?

Because of what is in it. 625 contains 58% minimum nickel, 20–23% chromium, 8–10% molybdenum and 3.15–4.15% niobium plus tantalum. Nickel and molybdenum are the two largest cost lines, and both are exchange-traded commodities. A 316L heats with roughly 10–12% nickel and 2–3% molybdenum, so the raw-material base alone is several times lower.

Does Inconel 625 price change with the LME nickel price?

Yes, and the relationship is direct. Every USD 1,000/t move on LME nickel shifts the nickel content of one kilogram of 625 by about USD 0.58. Molybdenum, niobium and chromium move independently, so the total can diverge from nickel alone. That is why suppliers quote with a validity window rather than a fixed catalogue price.

What is the difference between an FOB price and a landed cost?

FOB covers the material loaded at the Chinese port. Landed cost adds ocean or air freight, insurance, import duty in your country, port and clearance charges, and any third-party inspection you require. On heavy alloy shipments freight is a small share; on small parcels it can dominate. Always compare quotes on the same Incoterm and the same test scope.

Is a cheaper Inconel 625 quote safe to accept?

Only after you normalise what is included. A quote can be lower because the heat is ESR rather than VAR, because the material is off-spec on niobium, because the mill test certificate is a copy rather than an original to EN 10204 3.1, because tolerances are commercial rather than precision, or because the validity window is unrealistically long. Compare chemistry against ASTM B443/B444/B446 and ask which melting route was used.

What does VAR versus ESR do to the price?

Vacuum arc remelting and electroslag remelting both improve cleanliness and homogeneity over air melting, but VAR carries a higher conversion cost and is normally specified for aerospace and nuclear duty under AMS 5666. If your application is chemical or marine rather than flight-critical, ESR or air-melted material to ASTM may be sufficient and materially cheaper. Decide the melting route before you compare prices.

How much does the size and tolerance of the part affect the price?

Significantly. A 20–60 mm hot-rolled bar is a standard mill product; a 300 mm forged ring with 0.1 mm concentricity is a bespoke forging with machining, extra ultrasonic testing and higher scrap. As a rule, the further the item moves from a catalogue mill form towards a finished machined component, the more the price is driven by process hours rather than by metal content.

What should I send to get an accurate Inconel 625 quote?

Product form, size or drawing, quantity with unit (pieces, kg or metres), the governing standard (ASTM B443, B444, B446 or AMS 5666), required test scope and certificate level, delivery Incoterm and destination port, and any NACE MR0175 or third-party inspection requirement. With those six items a mill can price without a second round of questions.

Can Inconel 625 be supplied to NACE MR0175 for sour service?

Yes. 625 is listed for sour service under NACE MR0175 / ISO 15156, subject to the hardness and heat-treatment conditions in the standard. State the requirement on the enquiry, because it adds hardness verification and documentation that are not part of a standard ASTM B446 order.

Is Inconel 625 ever the wrong choice on cost grounds?

Frequently. If the service is below roughly 400 °C with no chlorides, 316L or 304L will do the same job at a quarter of the metal cost. If the duty is sulphuric or phosphoric acid at moderate temperature, Incoloy 825 is usually adequate. 625 earns its premium where seawater, chlorides and temperatures up to 980 °C coincide, or where the part must be welded in place without post-weld heat treatment.

Put your own numbers against this page

Send form, size, quantity and standard, and you get a priced reply with the melting route, certificate level and validity window stated — so it can be compared with any other quote on the same basis.

Request an Inconel 625 quote
Request a Quote
Add RAS Thermal as a preferred source on Google