Inconel 625
Ni-Cr-Mo alloy with outstanding corrosion resistance and high strength from cryogenic to 980°C.
Introduction
§01, GeneralNo heat treatment, no aging, just 8-10% molybdenum and niobium doing solid-solution work from cryogenic temperatures to 980°C. 625 resists pitting, crevice attack and stress-corrosion cracking in seawater and chemical duty, and it welds without post-weld treatment. Seawater, chemical processing, aerospace: the generalist that beats specialists in half of them.
Cross-Reference
Quick Facts
- UNS
- N06625
- GB
- GH3625
- Density
- 8.44 g/cm³
- Max Service Temp
- 980°C
- Series
- Inconel
Chemical Composition
ASTM B443 / B444 / B446 (N06625), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | 58.0 min (balance) | Base matrix; corrosion resistance |
| Chromium | Cr | 20.0 – 23.0 | Oxidation & pitting resistance |
| Molybdenum | Mo | 8.0 – 10.0 | Crevice corrosion resistance; strengthening |
| Niobium + Tantalum | Nb+Ta | 3.15 – 4.15 | Matrix stiffening with Mo |
| Iron | Fe | 5.0 max | Controlled residual |
| Carbon | C | 0.10 max | Carbide control |
| Manganese | Mn | 0.50 max | Deoxidiser |
| Silicon | Si | 0.50 max | Deoxidiser |
| Phosphorus | P | 0.015 max | Controlled residual |
| Sulfur | S | 0.015 max | Controlled residual |
| Aluminum | Al | 0.40 max | Controlled residual |
| Titanium | Ti | 0.40 max | Controlled residual |
| Cobalt | Co | 1.0 max | Controlled residual |
Mechanical & Physical Properties
ASTM B443 Gr.1, annealed, room temperature
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | 827 MPa min | Annealed, RT (Gr.1) |
| Yield Strength (0.2% offset) | 414 MPa min | Annealed, RT |
| Elongation | 30% min | Annealed, RT |
| Density | 8.44 g/cm³ | Physical |
| Melting Range | 1290–1350 °C | Physical |
| Max Service Temperature | 980 °C | Oxidising atmosphere |
Applicable Standards & Product Forms
Inconel 625 · UNS N06625 · GB/T GH3625
| Standard | Product Form |
|---|---|
| ASTM B443 | Plate, Sheet & Strip |
| ASTM B444 | Bar |
| ASTM B446 | Rod |
| AMS 5666 | Aerospace forgings / bar |
| NACE MR0175 | Sour service compliance |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Inconel Grades
Rated 1100°C, higher than this grade, also used for processing, same Inconel series.
Rated 1095°C, higher than this grade, also used for processing, same Inconel series.
Rated 1100°C, higher than this grade, also used for nuclear, same Inconel series.
Rated 1000°C, in the same class as this grade, same Inconel series.
Related Nickel Alloys
Rated 650°C, lower than this grade, also used for chemical, from the Hastelloy series.
Rated 650°C, lower than this grade, also used for processing, from the Hastelloy series.
Rated 540°C, lower than this grade, also used for processing, from the Monel series.
Cost guide
What does Inconel 625 cost per kg?
How the price is built: the LME nickel linkage behind the metal floor, where each form sits on cost, and the six variables that explain why two quotes for the same tonnage can differ by 40%.
Pricing
How Inconel 625 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
What can be stated precisely is the nickel floor: at 58% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Inconel 625 is about USD 8.88. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Inconel 625 FAQWhat is Inconel 625 used for?
Inconel 625 is a Inconel alloy used in Seawater piping and risers, Chemical processing equipment, Aircraft ducting systems. It offers Excellent pitting and crevice corrosion resistance and Oxidation resistant to 980°C.
What is the chemical composition of Inconel 625?
Inconel 625 is a controlled-composition Inconel alloy supplied to ASTM B443 and ASTM B444. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Inconel 625 available in?
Inconel 625 is regularly supplied in Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.
What is the maximum service temperature of Inconel 625?
Inconel 625 is rated for service up to 980°C. Contact our metallurgy team for specific application recommendations.
Need Inconel 625 material?
Request a quote with your specification: grade, form, dimensions and quantity.