Hastelloy B-3
Third-generation Ni-Mo alloy with maximized thermal stability and fabricability.
Introduction
§01, GeneralThird generation, and it shows. Hastelloy B-3 suppresses the Ni₃Mo and Ni₄Mo phases that made earlier B grades prone to intergranular corrosion after fabrication, so you can weld and hot form without that risk. HCl resistance stays at the level the B family is known for.
Cross-Reference
Quick Facts
- UNS
- N10675
- Density
- 9.22 g/cm³
- Max Service Temp
- 650°C
- Series
- Hastelloy
Chemical Composition
Haynes B-3 datasheet (N10675), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | Balance (65 min) | Base matrix |
| Molybdenum | Mo | 26.5 – 30.5 | HCl resistance; improved thermal stability vs B-2 |
| Iron | Fe | 1.0 – 3.0 | Controlled addition |
| Chromium | Cr | 1.5 max | Strictly limited |
| Cobalt | Co | 0.20 max | Controlled residual |
| Carbon | C | 0.01 max | Carbide control |
| Manganese | Mn | 3.0 max | Deoxidiser |
Mechanical & Physical Properties
Haynes B-3 datasheet, typical (annealed)
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | 800 MPa min | Typical, annealed RT |
| Yield Strength (0.2% offset) | 345 MPa min | Typical, annealed RT |
| Elongation | 43% min | Typical, annealed RT |
| Density | 9.22 g/cm³ | Physical |
Applicable Standards & Product Forms
Hastelloy B-3 · UNS N10675 · GB/T —
| Standard | Product Form |
|---|---|
| ASTM B333 | Plate, Sheet & Strip |
| ASTM B335 | Plate, Sheet & Strip |
| ASTM B366 | Fittings |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Hastelloy Grades
Rated 650°C, in the same class as this grade, also used for pharmaceutical, same Hastelloy series.
Rated 600°C, in the same class as this grade, also used for synthesis, same Hastelloy series.
Rated 650°C, in the same class as this grade, also used for pharmaceutical, same Hastelloy series.
Rated 600°C, in the same class as this grade, also used for pharmaceutical, same Hastelloy series.
Related Nickel Alloys
Rated 540°C, lower than this grade, also used for chemical, from the Incoloy series.
Rated 540°C, lower than this grade, also used for chemical, from the Monel series.
Rated 650°C, in the same class as this grade, from the Incoloy series.
Pricing
How Hastelloy B-3 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
What can be stated precisely is the nickel floor: at 65% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Hastelloy B-3 is about USD 9.95. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Hastelloy B-3 FAQWhat is Hastelloy B-3 used for?
Hastelloy B-3 is a Hastelloy alloy used in HCl absorber columns, Chemical reactor internals, Acid regeneration systems. It offers Maximized thermal stability and Eliminates Ni₃Mo/Ni₄Mo embrittlement.
What is the chemical composition of Hastelloy B-3?
Hastelloy B-3 is a controlled-composition Hastelloy alloy supplied to ASTM B333 and ASTM B335. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Hastelloy B-3 available in?
Hastelloy B-3 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.
What is the maximum service temperature of Hastelloy B-3?
Hastelloy B-3 is rated for service up to 650°C. Contact our metallurgy team for specific application recommendations.
Need Hastelloy B-3 material?
Request a quote with your specification: grade, form, dimensions and quantity.