Hastelloy C22 alloy products
Material Family / Hastelloy

Hastelloy C22

Ni-Cr-Mo-W alloy with superior oxidizing media resistance and better weldability than C-276.

Introduction

§01, General

Oxidizing media is where C22 pulls ahead of C-276, and it welds more easily too. The Ni-Cr-Mo-W chemistry covers both oxidizing and reducing environments, which suits flue gas desulfurization systems and pharmaceutical processing. When a vessel sees mixed duty, this is the upgrade path.

Cross-Reference

UNS: UNS N06022
Series: Hastelloy
Density: 8.69 g/cm³
Max Temp: 600°C
Standards: ASME Section VIII · ASTM B574 · ASTM B575 · NACE MR0175

Quick Facts

UNS
N06022
Density
8.69 g/cm³
Max Service Temp
600°C
Series
Hastelloy

Chemical Composition

ASTM B574 / B575 (N06022), wt%

Element Symbol Content (wt%) Role
Nickel Ni Balance Base matrix
Chromium Cr 20.0 – 22.5 Oxidizing-media resistance
Molybdenum Mo 12.5 – 14.5 Reducing-media resistance
Iron Fe 2.0 – 6.0 Controlled addition
Tungsten W 2.5 – 3.5 Strengthening
Vanadium V 0.35 max Controlled residual
Cobalt Co 2.5 max Controlled residual
Carbon C 0.015 max Grain-boundary carbide control

Mechanical & Physical Properties

ASTM B574, annealed, room temperature

Property Value Condition
Tensile Strength 690 MPa min Annealed, RT
Yield Strength (0.2% offset) 310 MPa min Annealed, RT
Elongation 45% min Annealed, RT
Density 8.69 g/cm³ Physical

Applicable Standards & Product Forms

Hastelloy C22 · UNS N06022 · GB/T —

Standard Product Form
ASTM B574 Bar
ASTM B575 Plate, Sheet & Strip
ASME Section VIII Pressure vessel code use
NACE MR0175 Sour service compliance
ForgingWireFlangeBar & RodPlate & SheetPipe & Tube

Available Product Forms

§02, Forms
ForgingWireFlangeBar & RodPlate & SheetPipe & Tube

Key Characteristics

§03, Features
Superior oxidizing media resistance
Better weldability than C-276
Resists pitting and crevice corrosion
ASME pressure vessel approved
Excellent in mixed acid environments

Typical Uses

§04, Applications
Flue gas desulfurization (FGD) scrubbers
Pharmaceutical processing equipment
Chemical reactor vessels
Pulp and paper bleach plants
Waste treatment systems

Pricing

How Hastelloy C22 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

Hastelloy C22 FAQ

What is Hastelloy C22 used for?

Hastelloy C22 is a Hastelloy alloy used in Flue gas desulfurization (FGD) scrubbers, Pharmaceutical processing equipment, Chemical reactor vessels. It offers Superior oxidizing media resistance and Better weldability than C-276.

What is the chemical composition of Hastelloy C22?

Hastelloy C22 is a controlled-composition Hastelloy alloy supplied to ASME Section VIII and ASTM B574. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is Hastelloy C22 available in?

Hastelloy C22 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.

What is the maximum service temperature of Hastelloy C22?

Hastelloy C22 is rated for service up to 600°C. Contact our metallurgy team for specific application recommendations.

Need Hastelloy C22 material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google