Incoloy 825
Ni-Fe-Cr-Mo-Cu alloy with exceptional resistance to sulfuric and phosphoric acid corrosion.
Introduction
§01 — GeneralIncoloy 825 is a nickel-iron-chromium alloy with additions of molybdenum, copper and titanium for exceptional corrosion resistance in reducing and oxidizing acids. It is the standard material for sulfuric acid coolers, phosphoric acid evaporators and chemical processing equipment handling mixed acid streams.
Cross-Reference
Quick Facts
- UNS
- N08825
- GB
- NS1402
- Density
- 8.14 g/cm³
- Max Service Temp
- 540°C
- Series
- Incoloy
Available Product Forms
§02 — FormsKey Characteristics
§03 — FeaturesTypical Uses
§04 — ApplicationsFrequently Asked Questions
Incoloy 825 FAQWhat is Incoloy 825 used for?
Incoloy 825 is a Incoloy alloy used in Sulfuric acid coolers, Phosphoric acid evaporators, Chemical reactor vessels. It offers Outstanding sulfuric acid resistance and Resistant to phosphoric acid.
What is the chemical composition of Incoloy 825?
Incoloy 825 is a controlled-composition Incoloy alloy supplied to ASTM B163 and ASTM B423. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Incoloy 825 available in?
Incoloy 825 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube. Custom forms and dimensions available on request.
What is the maximum service temperature of Incoloy 825?
Incoloy 825 is rated for service up to 540°C. Contact our metallurgy team for specific application recommendations.