Incoloy 800
Ni-Fe-Cr alloy for high-temperature heat exchangers and process piping in petrochemical plants.
Introduction
§01, GeneralHigh iron content keeps the price down, and 800 still carries good strength plus oxidation and carburization resistance from 600°C to 1100°C. Petrochemical furnace tubes, heat exchangers and process piping consume most of it. At 7.94 g/cm³ it's also one of the lighter nickel alloys in the catalog.
Cross-Reference
Quick Facts
- UNS
- N08800
- GB
- NS111
- Density
- 7.94 g/cm³
- Max Service Temp
- 1100°C
- Series
- Incoloy
Chemical Composition
ASTM B408 / B163 (N08800), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | 30.0 – 35.0 | Carburization resistance |
| Chromium | Cr | 19.0 – 23.0 | Oxidation resistance |
| Aluminum | Al | 0.15 – 0.60 | Oxide scale control |
| Titanium | Ti | 0.15 – 0.60 | Oxide scale control |
| Carbon | C | 0.12 max | Controlled residual |
| Manganese | Mn | 1.5 max | Deoxidiser |
| Silicon | Si | 1.0 max | Controlled residual |
| Copper | Cu | 0.75 max | Controlled residual |
| Iron | Fe | Balance | Base |
Mechanical & Physical Properties
ASTM B408, annealed, room temperature
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | 515 MPa min | Annealed, RT |
| Yield Strength (0.2% offset) | 205 MPa min | Annealed, RT |
| Elongation | 30% min | Annealed, RT |
| Density | 7.94 g/cm³ | Physical |
Applicable Standards & Product Forms
Incoloy 800 · UNS N08800 · GB/T NS111
| Standard | Product Form |
|---|---|
| ASTM B163 | Seamless heat-exchanger tube |
| ASTM B407 | Seamless Pipe & Tube |
| ASTM B408 | Bar & Rod |
| ASME SB-407 | ASME code pipe & tube |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Incoloy Grades
Rated 1100°C, in the same class as this grade, also used for petrochemical, same Incoloy series.
Rated 1100°C, in the same class as this grade, also used for ethylene, same Incoloy series.
Rated 700°C, lower than this grade; this grade is additionally offered as pipe, same Incoloy series.
Rated 650°C, lower than this grade, same Incoloy series.
Related Nickel Alloys
Rated 1095°C, in the same class as this grade, also used for ethylene, from the Inconel series.
Rated 1100°C, in the same class as this grade, also used for petrochemical, from the Hastelloy series.
Rated 1100°C, in the same class as this grade, also used for petrochemical, from the Inconel series.
Pricing
How Incoloy 800 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
What can be stated precisely is the nickel floor: at 30% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Incoloy 800 is about USD 4.59. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Incoloy 800 FAQWhat is Incoloy 800 used for?
Incoloy 800 is a Incoloy alloy used in Ethylene furnace tubes, Heat exchanger bundles, Steam superheater tubing. It offers Cost-effective vs Inconel and Good oxidation resistance to 1100°C.
What is the chemical composition of Incoloy 800?
Incoloy 800 is a controlled-composition Incoloy alloy supplied to ASTM B163 and ASTM B407. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Incoloy 800 available in?
Incoloy 800 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube. Custom forms and dimensions available on request.
What is the maximum service temperature of Incoloy 800?
Incoloy 800 is rated for service up to 1100°C. Contact our metallurgy team for specific application recommendations.
Need Incoloy 800 material?
Request a quote with your specification: grade, form, dimensions and quantity.