Inconel 617 alloy products
Material Family / Inconel

Inconel 617

Ni-Cr-Co-Mo alloy with outstanding creep strength at high temperatures for power generation.

Introduction

§01, General

Cobalt and molybdenum in solid solution buy creep strength few alloys match. 617 is the alloy of choice for ultra-supercritical power plant boiler tubes, with oxidation resistance that holds on the fire side too. Power engineers spec it when nothing cheaper survives the steam conditions, and its 1100°C ceiling leaves margin.

Cross-Reference

UNS: UNS N06617
GB/T: GB NS3303
Series: Inconel
Density: 8.36 g/cm³
Max Temp: 1100°C
Standards: ASTM B166 · ASTM B167 · ASME SB-167 · AMS 5887

Quick Facts

UNS
N06617
GB
NS3303
Density
8.36 g/cm³
Max Service Temp
1100°C
Series
Inconel

Chemical Composition

ASTM B166 / B167 (N06617), wt%

Element Symbol Content (wt%) Role
Nickel Ni Balance (44.5 min) Base matrix
Chromium Cr 20.0 – 24.0 Oxidation resistance
Cobalt Co 10.0 – 15.0 Phase stability
Molybdenum Mo 8.0 – 10.0 Solid-solution strengthening
Aluminum Al 0.8 – 1.5 Oxide scale control
Titanium Ti 0.6 max Controlled residual
Carbon C 0.05 – 0.15 Carbide strengthening
Iron Fe 3.0 max Controlled residual

Mechanical & Physical Properties

Manufacturer datasheet, typical (solution annealed)

Property Value Condition
Tensile Strength 690 MPa Typical, annealed RT
Yield Strength (0.2% offset) 300 MPa Typical, annealed RT
Elongation 40% Typical, annealed RT
Density 8.36 g/cm³ Physical

Applicable Standards & Product Forms

Inconel 617 · UNS N06617 · GB/T —

Standard Product Form
ASTM B166 Rod & Bar
ASTM B167 Seamless Pipe & Tube
ASME SB-167 ASME code pipe & tube
AMS 5887 Forgings
ForgingWireFlangeBar & RodPlate & SheetPipe & Tube

Available Product Forms

§02, Forms
ForgingWireFlangeBar & RodPlate & SheetPipe & Tube

Key Characteristics

§03, Features
Exceptional creep strength
Oxidation resistant to 1100°C
Carburization resistant
Good weldability
Power generation grade qualified

Typical Uses

§04, Applications
Ultra-supercritical boiler tubes
Gas turbine transition ducts
Nuclear reactor components
Heat-treating furnace hardware
Petrochemical cracking tubes

Pricing

How Inconel 617 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

What can be stated precisely is the nickel floor: at 44.5% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Inconel 617 is about USD 6.81. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

Inconel 617 FAQ

What is Inconel 617 used for?

Inconel 617 is a Inconel alloy used in Ultra-supercritical boiler tubes, Gas turbine transition ducts, Nuclear reactor components. It offers Exceptional creep strength and Oxidation resistant to 1100°C.

What is the chemical composition of Inconel 617?

Inconel 617 is a controlled-composition Inconel alloy supplied to ASTM B166 and ASTM B167. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is Inconel 617 available in?

Inconel 617 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.

What is the maximum service temperature of Inconel 617?

Inconel 617 is rated for service up to 1100°C. Contact our metallurgy team for specific application recommendations.

Need Inconel 617 material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google