Inconel 690 alloy products
Material Family / Inconel

Inconel 690

High-chromium Ni-Cr-Fe alloy for nuclear steam generator tubing with superior SCC resistance.

Introduction

§01, General

30% chromium, roughly double Alloy 600's level, is the whole story. 690 resists stress-corrosion cracking in high-temperature water so well that it became the industry standard for PWR steam generator tubing. When a plant replaces 600 tubing, this 8.19 g/cm³ alloy is what goes in.

Cross-Reference

UNS: UNS N06690
GB/T: GB NS3105
Series: Inconel
Density: 8.19 g/cm³
Max Temp: 1100°C
Standards: ASTM B166 · ASTM B167 · ASTM B168 · ASME N-Stamp

Quick Facts

UNS
N06690
GB
NS3105
Density
8.19 g/cm³
Max Service Temp
1100°C
Series
Inconel

Chemical Composition

ASTM B166 / B167 (N06690), wt%

Element Symbol Content (wt%) Role
Nickel Ni 58.0 min Base matrix; primary-water resistance
Chromium Cr 27.0 – 31.0 High Cr for nuclear duty
Iron Fe 7.0 – 11.0 Controlled addition
Carbon C 0.05 max Controlled residual
Manganese Mn 0.5 max Deoxidiser
Silicon Si 0.5 max Controlled residual
Copper Cu 0.5 max Controlled residual

Mechanical & Physical Properties

Manufacturer datasheet, typical (annealed)

Property Value Condition
Tensile Strength 585 MPa Typical, annealed RT
Yield Strength (0.2% offset) 240 MPa Typical, annealed RT
Elongation 30% Typical, annealed RT
Density 8.19 g/cm³ Physical

Applicable Standards & Product Forms

Inconel 690 · UNS N06690 · GB/T NS3105

Standard Product Form
ASTM B166 Rod & Bar
ASTM B167 Seamless Pipe & Tube
ASTM B168 Plate, Sheet & Strip
ASME N-Stamp Nuclear component use
ForgingWireFlangeBar & RodPlate & SheetPipe & Tube

Available Product Forms

§02, Forms
ForgingWireFlangeBar & RodPlate & SheetPipe & Tube

Key Characteristics

§03, Features
Best-in-class SCC resistance
30% Cr for nuclear water chemistry
PWR steam generator standard
Resistant to caustic environments
ASME nuclear qualified

Typical Uses

§04, Applications
Nuclear steam generator tubing
Nuclear waste vitrification
Chemical processing equipment
Coal gasification systems
Incinerator components

Pricing

How Inconel 690 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

What can be stated precisely is the nickel floor: at 58% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Inconel 690 is about USD 8.88. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

Inconel 690 FAQ

What is Inconel 690 used for?

Inconel 690 is a Inconel alloy used in Nuclear steam generator tubing, Nuclear waste vitrification, Chemical processing equipment. It offers Best-in-class SCC resistance and 30% Cr for nuclear water chemistry.

What is the chemical composition of Inconel 690?

Inconel 690 is a controlled-composition Inconel alloy supplied to ASTM B166 and ASTM B167. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is Inconel 690 available in?

Inconel 690 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.

What is the maximum service temperature of Inconel 690?

Inconel 690 is rated for service up to 1100°C. Contact our metallurgy team for specific application recommendations.

Need Inconel 690 material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google