Spools of nickel alloy spring wire on a precision winding machine
Product FormDoc. RAS·WIRE & SPRING WIRE/01

Precision Alloy Wire

From Ø0.10 mm fine wire to 12.0 mm spring stock, cold drawn and supplied in coil, spool or cut lengths.

Wire & Spring Wire Capabilities

§01, Overview

Wire is where tolerance discipline shows. We draw nickel, cobalt and precipitation-hardening alloys to exact diameter and mechanical properties, hold tensile within ±50 MPa typical, and ship spring wire bright or oxidized with certification for high-cycle and high-temperature springs.

ASTM B637ASTM B574ASTM B164AMS 5662AMS 5708

Key Capabilities

Diameter range
Ø0.10 - 12.0 mm
Coil weight
Up to 500 kg
Spool types
DIN 160, DIN 250, DIN 355, K125 / K250
Finish
Bright, oxidized, coated, skin-pass
Packaging
Vacuum / inert gas on request

Why RAS Thermal

§02, Quality + Traceability
Tight diameter tolerance and ovality control
Tensile and coil-set properties held uniform across the coil
Bright or oxidized surface, ready for spring coiling
Cut-to-length and spooled delivery
Mill test certificate with every batch

Sizes & Tolerances

§03, Specifications
TypeRangeNote
Spring wireØ0.15 - 12.0 mmCoil / spool / cut
Cold-drawn wireØ0.10 - 10.0 mmCoil / spool / straight
Welding wireØ0.8 - 4.0 mmSpool

Tolerances

Diameter
h9 / h10 / per customer spec
Tensile
±50 MPa typical
Surface
No visible defects, bright / oxidized

Typical End Uses

§04, Applications
High-temperature springs
Corrosion-resistant springs
Welding filler wire
Medical guidewires
Fastener and mesh wire

Frequently Asked Questions

Wire & Spring Wire FAQ

What diameter tolerance do you hold on Inconel 718 spring wire?

Ø0.10 mm to 12.0 mm, h9/h10 on diameter, ±50 MPa typical on tensile. Supplied bright or oxidized in coil, DIN 160/250/355 or K125/K250 spools up to 500 kg.

Which alloys and standards cover your wire products?

Inconel 718 and X-750 run under ASTM B637 with AMS 5662 and AMS 5698, Hastelloy C-276 under ASTM B574, Monel 400 and K-500 under ASTM B164. Every batch carries an MTC listing chemistry, tensile values and heat number.

Do you supply welding wire and medical guidewire stock?

Yes. Welding filler wire comes from Ø0.8 to 4.0 mm on spools, and medical guidewire stock draws down to Ø0.10 mm in MP35N and corrosion-resistant grades. Vacuum or inert-gas packaging on request.

Technical Enquiry

Request a Wire & Spring Wire quote

Request a Quote
Add RAS Thermal as a preferred source on Google