Hastelloy X alloy products
Material Family / Hastelloy

Hastelloy X

Ni-Cr-Fe-Mo alloy for combustion zone components with exceptional oxidation resistance to 1100°C.

Introduction

§01, General

Combustion chambers, afterburner components, furnace hardware past 1000°C: Hastelloy X is the standard there for a reason. The Ni-Cr-Fe-Mo chemistry holds strength and resists oxidation to 1100°C, and it sheet-forms well enough to make complicated hot-section hardware practical.

Cross-Reference

UNS: UNS N06002
GB/T: GB GH3536
Series: Hastelloy
Density: 8.22 g/cm³
Max Temp: 1100°C
Standards: AMS 5536 · AMS 5754 · ASTM B435 · ASTM B572

Quick Facts

UNS
N06002
GB
GH3536
Density
8.22 g/cm³
Max Service Temp
1100°C
Series
Hastelloy

Chemical Composition

ASTM B435 / B572 + AMS 5536 (N06002), wt%

Element Symbol Content (wt%) Role
Nickel Ni Balance Base matrix
Chromium Cr 20.5 – 23.0 Oxidation resistance
Iron Fe 17.0 – 20.0 Controlled addition
Molybdenum Mo 8.0 – 10.0 Strengthening
Cobalt Co 0.5 – 2.5 Strengthening
Tungsten W 0.2 – 1.0 Strengthening
Carbon C 0.05 – 0.15 Carbide strengthening

Mechanical & Physical Properties

ASTM B435, annealed, room temperature

Property Value Condition
Tensile Strength 655 MPa min Annealed, RT
Yield Strength (0.2% offset) 275 MPa min Annealed, RT
Elongation 35% min Annealed, RT
Density 8.22 g/cm³ Physical
Max Service Temperature 1100 °C Furnace & combustor duty

Applicable Standards & Product Forms

Hastelloy X · UNS N06002 · GB/T GH3536

Standard Product Form
AMS 5536 Sheet & strip (aerospace)
AMS 5754 Bar & forgings (aerospace)
ASTM B435 Plate, Sheet & Strip
ASTM B572 Bar & Rod
ForgingWireFlangeBar & RodPlate & SheetPipe & Tube

Available Product Forms

§02, Forms
ForgingWireFlangeBar & RodPlate & SheetPipe & Tube

Key Characteristics

§03, Features
Oxidation resistant to 1100°C
Excellent high-temperature strength
Good fabricability
Resistant to carburization and nitriding
Combustion zone standard material

Typical Uses

§04, Applications
Gas turbine combustion chambers
Afterburner components
Industrial furnace hardware
Heat-treating equipment
Petrochemical cracking tubes

Selection guide

Is Hastelloy X the right grade for your temperature?

Side-by-side specification comparison with GH3044 and Inconel 625, including the service temperature at which each stops being the correct purchase.

Compare the three →

Pricing

How Hastelloy X is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

Hastelloy X FAQ

What is Hastelloy X used for?

Hastelloy X is a Hastelloy alloy used in Gas turbine combustion chambers, Afterburner components, Industrial furnace hardware. It offers Oxidation resistant to 1100°C and Excellent high-temperature strength.

What is the chemical composition of Hastelloy X?

Hastelloy X is a controlled-composition Hastelloy alloy supplied to AMS 5536 and AMS 5754. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is Hastelloy X available in?

Hastelloy X is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.

What is the maximum service temperature of Hastelloy X?

Hastelloy X is rated for service up to 1100°C. Contact our metallurgy team for specific application recommendations.

Need Hastelloy X material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google