Inconel 601 alloy products
Material Family / Inconel

Inconel 601

Ni-Cr-Fe alloy with aluminum addition for superior oxidation resistance to 1180°C.

Introduction

§01, General

Aluminum changes everything. 601 grows a tenacious aluminum oxide scale that survives cyclic heating, pushing oxidation resistance to 1180°C. Furnace components and radiant tubes that see repeated thermal shocks are the classic applications.

Cross-Reference

UNS: UNS N06601
GB/T: GB NS3103
Series: Inconel
Density: 8.11 g/cm³
Max Temp: 1180°C
Standards: ASTM B166 · ASTM B167 · ASTM B168 · AMS 5715

Quick Facts

UNS
N06601
GB
NS3103
Density
8.11 g/cm³
Max Service Temp
1180°C
Series
Inconel

Chemical Composition

ASTM B166 / B168 (N06601), wt%

Element Symbol Content (wt%) Role
Nickel Ni 58.0 – 63.0 Base matrix
Chromium Cr 21.0 – 25.0 Oxidation & spalling resistance
Aluminum Al 1.0 – 1.7 Adherent oxide scale
Carbon C 0.10 max Controlled residual
Manganese Mn 1.0 max Deoxidiser
Silicon Si 0.5 max Controlled residual
Copper Cu 1.0 max Controlled residual
Iron Fe Balance Base

Mechanical & Physical Properties

ASTM B168, annealed, room temperature

Property Value Condition
Tensile Strength 550 MPa min Annealed, RT
Yield Strength (0.2% offset) 205 MPa min Annealed, RT
Elongation 30% min Annealed, RT
Density 8.11 g/cm³ Physical
Melting Range 1360–1411 °C Physical

Applicable Standards & Product Forms

Inconel 601 · UNS N06601 · GB/T NS3103

Standard Product Form
ASTM B166 Rod & Bar
ASTM B167 Seamless Pipe & Tube
ASTM B168 Plate, Sheet & Strip
AMS 5715 Bar & forgings (aerospace)
ForgingWireFlangeBar & RodPlate & SheetStripPipe & Tube

Available Product Forms

§02, Forms
ForgingWireFlangeBar & RodPlate & SheetStripPipe & Tube

Key Characteristics

§03, Features
Oxidation resistant to 1180°C
Excellent thermal cycling resistance
Forms protective Al₂O₃ scale
Good in carburizing environments
Spall-resistant oxide layer

Typical Uses

§04, Applications
Radiant furnace tubes
Heat-treating baskets and fixtures
Combustion chamber components
Thermal oxidizer systems
Petrochemical reformers

Pricing

How Inconel 601 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

What can be stated precisely is the nickel floor: at 58% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Inconel 601 is about USD 8.88. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

Inconel 601 FAQ

What is Inconel 601 used for?

Inconel 601 is a Inconel alloy used in Radiant furnace tubes, Heat-treating baskets and fixtures, Combustion chamber components. It offers Oxidation resistant to 1180°C and Excellent thermal cycling resistance.

What is the chemical composition of Inconel 601?

Inconel 601 is a controlled-composition Inconel alloy supplied to ASTM B166 and ASTM B167. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is Inconel 601 available in?

Inconel 601 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube. Custom forms and dimensions available on request.

What is the maximum service temperature of Inconel 601?

Inconel 601 is rated for service up to 1180°C. Contact our metallurgy team for specific application recommendations.