Inconel 693
Advanced Ni-Cr-Al alloy with unparalleled metal dusting resistance for petrochemical reforming.
Introduction
§01, GeneralMetal dusting eats conventional alloys in CO-rich syngas. 693, a high-chromium Ni-Cr-Al chemistry, was built for exactly that environment and leads the field in metal dusting and carburization resistance. Hydrogen and syngas plants specify it for the spots where everything else turns to powder.
Cross-Reference
Quick Facts
- UNS
- N06693
- Density
- 8.2 g/cm³
- Max Service Temp
- 1000°C
- Series
- Inconel
Chemical Composition
Special Metals datasheet (N06693), nominal wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | Balance | Base matrix |
| Chromium | Cr | 27.0 – 31.0 | Oxidation resistance |
| Iron | Fe | 7.0 – 11.0 | Controlled addition |
| Aluminum | Al | 2.7 – 3.7 | Sulfidation resistance |
| Titanium | Ti | 0.7 – 1.3 | γ′ strengthening |
| Niobium | Nb | 0.7 – 1.5 | γ′ strengthening |
| Carbon | C | 0.05 max | Controlled residual |
Mechanical & Physical Properties
Manufacturer datasheet, typical (annealed)
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | ≈700 MPa | Typical, annealed RT |
| Density | 8.2 g/cm³ | Physical |
Applicable Standards & Product Forms
Inconel 693 · UNS N06693 · GB/T —
| Standard | Product Form |
|---|---|
| ASTM B166 | Rod & Bar |
| ASTM B167 | Seamless Pipe & Tube |
| NACE TM0198 | Sour service testing |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Inconel Grades
Rated 1095°C, higher than this grade, also used for production, same Inconel series.
Rated 1100°C, higher than this grade, same Inconel series.
Rated 1100°C, higher than this grade, same Inconel series.
Rated 980°C, in the same class as this grade, same Inconel series.
Related Nickel Alloys
Rated 1100°C, higher than this grade, also used for methane, from the Incoloy series.
Rated 1100°C, higher than this grade, from the Incoloy series.
Rated 1100°C, higher than this grade, also used for reformer, from the Incoloy series.
Pricing
How Inconel 693 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Inconel 693 FAQWhat is Inconel 693 used for?
Inconel 693 is a Inconel alloy used in Steam methane reformer outlets, Syngas cooler tubes, Hydrogen production plants. It offers Unparalleled metal dusting resistance and Carburization resistant.
What is the chemical composition of Inconel 693?
Inconel 693 is a controlled-composition Inconel alloy supplied to ASTM B166 and ASTM B167. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Inconel 693 available in?
Inconel 693 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.
What is the maximum service temperature of Inconel 693?
Inconel 693 is rated for service up to 1000°C. Contact our metallurgy team for specific application recommendations.
Need Inconel 693 material?
Request a quote with your specification: grade, form, dimensions and quantity.