Hastelloy B-2
Low-carbon variant of Hastelloy B with improved weld zone corrosion resistance.
Introduction
§01, GeneralB-2 cuts the carbon and the iron out of the Hastelloy B chemistry, and the weld zones stop being the weak point. Knife-line attack and heat-affected-zone corrosion drop sharply, so many fabrications no longer need post-weld solution treatment. You keep the family's exceptional hydrochloric acid resistance and lose most of the welding headaches.
Cross-Reference
Quick Facts
- UNS
- N10665
- GB
- NS3202
- Density
- 9.22 g/cm³
- Max Service Temp
- 650°C
- Series
- Hastelloy
Chemical Composition
ASTM B335 / B333 / B564 (N10665), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | Balance (≈69 min) | Base matrix |
| Molybdenum | Mo | 26.0 – 30.0 | Hydrochloric acid resistance |
| Iron | Fe | 2.0 max | Controlled residual |
| Chromium | Cr | 1.0 max | Strictly limited |
| Carbon | C | 0.02 max | Low-C variant; weld-zone corrosion control |
| Cobalt | Co | 1.0 max | Controlled residual |
| Manganese | Mn | 1.0 max | Deoxidiser |
| Silicon | Si | 0.10 max | Strictly limited |
| Phosphorus | P | 0.040 max | Controlled residual |
| Sulfur | S | 0.030 max | Controlled residual |
| Vanadium | V | 0.20 max | Controlled residual |
Mechanical & Physical Properties
ASTM B335 / B574, annealed, room temperature
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | 760 MPa min | Annealed, RT |
| Yield Strength (0.2% offset) | 350 MPa min | Annealed, RT |
| Elongation | 40% min | Annealed, RT |
| Density | 9.22 g/cm³ | Physical |
| Melting Range | 1330–1380 °C | Physical |
| Max Service Temperature | 650 °C | Reducing media |
Applicable Standards & Product Forms
Hastelloy B-2 · UNS N10665 · GB/T NS3202
| Standard | Product Form |
|---|---|
| ASTM B335 | Plate, Sheet & Strip |
| ASTM B333 | Plate, Sheet & Strip |
| ASME SB-333 | Pressure vessel use |
| ASTM B366 | Fittings |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Hastelloy Grades
Rated 650°C, in the same class as this grade, also used for pharmaceutical, same Hastelloy series.
Rated 650°C, in the same class as this grade, also used for pharmaceutical, same Hastelloy series.
Rated 600°C, in the same class as this grade, also used for production, same Hastelloy series.
Rated 600°C, in the same class as this grade, same Hastelloy series.
Related Nickel Alloys
Rated 540°C, lower than this grade, also used for alkylation, from the Monel series.
Rated 540°C, lower than this grade, also used for production, from the Incoloy series.
Rated 650°C, in the same class as this grade, from the Incoloy series.
Pricing
How Hastelloy B-2 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
What can be stated precisely is the nickel floor: at 69% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Hastelloy B-2 is about USD 10.56. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Hastelloy B-2 FAQWhat is Hastelloy B-2 used for?
Hastelloy B-2 is a Hastelloy alloy used in HCl distillation columns, Acetic acid production, Ethyl benzene alkylation. It offers Improved weld zone corrosion resistance and No post-weld heat treat needed.
What is the chemical composition of Hastelloy B-2?
Hastelloy B-2 is a controlled-composition Hastelloy alloy supplied to ASTM B333 and ASTM B335. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Hastelloy B-2 available in?
Hastelloy B-2 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.
What is the maximum service temperature of Hastelloy B-2?
Hastelloy B-2 is rated for service up to 650°C. Contact our metallurgy team for specific application recommendations.
Need Hastelloy B-2 material?
Request a quote with your specification: grade, form, dimensions and quantity.