Hastelloy B
Ni-Mo alloy with outstanding resistance to hydrochloric acid at all concentrations and temperatures.
Introduction
§01, GeneralHydrochloric acid, any concentration, any temperature: Hastelloy B is the premier material for exactly that duty. The nickel-molybdenum chemistry has one weakness, oxidizing impurities, so ferric ions or dissolved oxygen in the acid need watching. Manage that and HCl equipment built from this 9.24 g/cm³ alloy runs for years.
Cross-Reference
Quick Facts
- GB
- NS3201
- Density
- 9.24 g/cm³
- Max Service Temp
- 650°C
- Series
- Hastelloy
Chemical Composition
ASTM B333 / B335 (Ni-Mo), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | Balance | Base; reducing-acid resistance |
| Molybdenum | Mo | 26.0 – 30.0 | Hydrochloric acid resistance |
| Iron | Fe | 4.0 – 7.0 | Controlled addition |
| Chromium | Cr | 1.0 max | Strictly limited |
| Carbon | C | 0.12 max | Weld-zone carbide risk (original B) |
| Manganese | Mn | 1.0 max | Deoxidiser |
| Silicon | Si | 1.0 max | Controlled residual |
Mechanical & Physical Properties
Manufacturer datasheet, typical (annealed)
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | 690 MPa min | Typical, annealed RT |
| Yield Strength (0.2% offset) | 310 MPa min | Typical, annealed RT |
| Elongation | 40% min | Typical, annealed RT |
| Density | 9.24 g/cm³ | Physical |
Applicable Standards & Product Forms
Hastelloy B · UNS — · GB/T NS3201
| Standard | Product Form |
|---|---|
| ASTM B333 | Plate, Sheet & Strip |
| ASTM B335 | Plate, Sheet & Strip |
| ASME SB-333 | Pressure vessel use |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Hastelloy Grades
Rated 650°C, in the same class as this grade, also used for pharmaceutical, same Hastelloy series.
Rated 600°C, in the same class as this grade, also used for processing, same Hastelloy series.
Rated 600°C, in the same class as this grade, also used for pharmaceutical, same Hastelloy series.
Rated 650°C, in the same class as this grade, also used for pharmaceutical, same Hastelloy series.
Related Nickel Alloys
Rated 540°C, lower than this grade, also used for chemical, from the Incoloy series.
Rated 540°C, lower than this grade, also used for processing, from the Monel series.
Rated 704°C, higher than this grade, also used for hardware, from the Inconel series.
Pricing
How Hastelloy B is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Hastelloy B FAQWhat is Hastelloy B used for?
Hastelloy B is a Hastelloy alloy used in Hydrochloric acid processing, Chemical reactor vessels, Vacuum furnace components. It offers Unmatched HCl resistance and All concentrations and temperatures.
What is the chemical composition of Hastelloy B?
Hastelloy B is a controlled-composition Hastelloy alloy supplied to ASTM B333 and ASTM B335. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Hastelloy B available in?
Hastelloy B is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.
What is the maximum service temperature of Hastelloy B?
Hastelloy B is rated for service up to 650°C. Contact our metallurgy team for specific application recommendations.