Hastelloy C-4
High-temperature stable Ni-Cr-Mo alloy free of intergranular precipitation for chemical equipment.
Introduction
§01, GeneralWeld it and run it. Hastelloy C-4 was designed to refuse grain-boundary precipitates during welding and elevated-temperature exposure, so chemical process equipment can operate in the as-welded condition with no post-weld heat treatment. Stability holds to 600°C.
Cross-Reference
Quick Facts
- UNS
- N06455
- GB
- NS3305
- Density
- 8.64 g/cm³
- Max Service Temp
- 600°C
- Series
- Hastelloy
Chemical Composition
ASTM B574 / B575 / B619 (N06455), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | Balance | Base matrix |
| Chromium | Cr | 14.5 – 17.5 | Oxidizing-media resistance |
| Molybdenum | Mo | 12.5 – 14.5 | Reducing-media resistance |
| Iron | Fe | 3.0 max | Controlled residual |
| Cobalt | Co | 2.5 max | Controlled residual |
| Titanium | Ti | 0.70 max | Stabilization |
| Carbon | C | 0.015 max | Grain-boundary carbide control |
| Manganese | Mn | 1.0 max | Deoxidiser |
| Silicon | Si | 0.08 max | Controlled residual |
Mechanical & Physical Properties
ASTM B574, annealed, room temperature
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | 690 MPa min | Annealed, RT |
| Yield Strength (0.2% offset) | 275 MPa min | Annealed, RT |
| Elongation | 40% min | Annealed, RT |
| Density | 8.64 g/cm³ | Physical |
Applicable Standards & Product Forms
Hastelloy C-4 · UNS N06455 · GB/T NS3305
| Standard | Product Form |
|---|---|
| ASTM B574 | Bar |
| ASTM B575 | Plate, Sheet & Strip |
| ASTM B619 | Welded Pipe & Tube |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Hastelloy Grades
Rated 650°C, in the same class as this grade, also used for synthesis, same Hastelloy series.
Rated 650°C, in the same class as this grade, also used for processing, same Hastelloy series.
Rated 650°C, in the same class as this grade, also used for production, same Hastelloy series.
Rated 600°C, in the same class as this grade, also used for chemical, same Hastelloy series.
Related Nickel Alloys
Rated 540°C, lower than this grade, also used for production, from the Incoloy series.
Rated 540°C, lower than this grade, also used for processing, from the Monel series.
Rated 650°C, in the same class as this grade, from the Incoloy series.
Pricing
How Hastelloy C-4 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Hastelloy C-4 FAQWhat is Hastelloy C-4 used for?
Hastelloy C-4 is a Hastelloy alloy used in Welded chemical vessels, Pesticide production equipment, Chlorinated organics processing. It offers No intergranular precipitation and As-welded operation.
What is the chemical composition of Hastelloy C-4?
Hastelloy C-4 is a controlled-composition Hastelloy alloy supplied to ASTM B574 and ASTM B575. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Hastelloy C-4 available in?
Hastelloy C-4 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.
What is the maximum service temperature of Hastelloy C-4?
Hastelloy C-4 is rated for service up to 600°C. Contact our metallurgy team for specific application recommendations.