Incoloy 925 alloy products
Material Family / Incoloy

Incoloy 925

Age-hardenable Incoloy for high-strength sour gas wellhead and downhole equipment.

Introduction

§01, General

Corrosion resistance like 825, then age-harden it. 925 precipitates to high strength while keeping the austenitic base's corrosion behavior, and it lands inside NACE MR0175 limits for sour service. Wellhead components, completion tools and downhole tubular hardware are its bread and butter.

Cross-Reference

UNS: UNS N09925
Series: Incoloy
Density: 8.14 g/cm³
Max Temp: 650°C
Standards: ASTM B805 · NACE MR0175 · API 6A

Quick Facts

UNS
N09925
Density
8.14 g/cm³
Max Service Temp
650°C
Series
Incoloy

Chemical Composition

ASTM B805 / Special Metals (N09925), wt%

Element Symbol Content (wt%) Role
Nickel Ni 42.0 – 46.0 Acid + sour-gas matrix
Chromium Cr 19.5 – 22.5 Oxidizing-media resistance
Molybdenum Mo 2.8 – 3.8 Pitting resistance
Copper Cu 1.5 – 3.0 Acid resistance
Titanium Ti 1.9 – 2.4 γ′ age hardening
Aluminum Al 0.1 – 0.5 γ′ age hardening
Iron Fe Balance Base

Mechanical & Physical Properties

Manufacturer datasheet, typical (aged)

Property Value Condition
Tensile Strength 900 MPa Typical, aged RT
Yield Strength (0.2% offset) 700 MPa Typical, aged RT
Elongation 20% Typical, aged RT
Density 8.14 g/cm³ Physical

Applicable Standards & Product Forms

Incoloy 925 · UNS N09925 · GB/T —

Standard Product Form
ASTM B805 Bar & Rod
NACE MR0175 Sour service compliance
API 6A Oilfield wellhead equipment
ForgingWireFlangeBar & Rod

Available Product Forms

§02, Forms
ForgingWireFlangeBar & Rod

Key Characteristics

§03, Features
Precipitation-hardenable to high strength
NACE MR0175 for sour service
API 6A wellhead qualified
Excellent in H₂S + CO₂ environments
Yield strength > 758 MPa achievable

Typical Uses

§04, Applications
Sour gas wellhead components
Downhole completion tools
High-strength fasteners
Gate valve stems and seats
Subsea Christmas tree components

Pricing

How Incoloy 925 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

What can be stated precisely is the nickel floor: at 42% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Incoloy 925 is about USD 6.43. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

Incoloy 925 FAQ

What is Incoloy 925 used for?

Incoloy 925 is a Incoloy alloy used in Sour gas wellhead components, Downhole completion tools, High-strength fasteners. It offers Precipitation-hardenable to high strength and NACE MR0175 for sour service.

What is the chemical composition of Incoloy 925?

Incoloy 925 is a controlled-composition Incoloy alloy supplied to ASTM B805 and NACE MR0175. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is Incoloy 925 available in?

Incoloy 925 is regularly supplied in Forging, Wire, Flange, Bar & Rod. Custom forms and dimensions available on request.

What is the maximum service temperature of Incoloy 925?

Incoloy 925 is rated for service up to 650°C. Contact our metallurgy team for specific application recommendations.

Need Incoloy 925 material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google