Incoloy A-286
Fe-Ni-Cr precipitation-hardenable alloy for high-temperature fasteners and automotive turbocharger springs.
Introduction
§01, GeneralA-286 is the value play for fastener duty to 700°C. An iron-nickel-chromium base strengthened by precipitation hardening delivers bolt and spring performance at a fraction of nickel-superalloy cost, which is why automotive turbochargers and aerospace casings consume it by the ton.
Cross-Reference
Quick Facts
- UNS
- S66286
- GB
- GH2132
- Density
- 7.94 g/cm³
- Max Service Temp
- 700°C
- Series
- Incoloy
Chemical Composition
AMS 5731 / ASTM A638 (S66286), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | 24.0 – 27.0 | Austenitic matrix |
| Chromium | Cr | 13.5 – 16.0 | Oxidation resistance |
| Molybdenum | Mo | 1.0 – 1.5 | Strengthening |
| Titanium | Ti | 1.9 – 2.35 | γ′ age hardening |
| Vanadium | V | 0.1 – 0.5 | Controlled addition |
| Aluminum | Al | 0.35 max | Controlled residual |
| Boron | B | 0.001 – 0.010 | Grain boundary control |
| Carbon | C | 0.08 max | Controlled residual |
| Iron | Fe | Balance | Base |
Mechanical & Physical Properties
ASTM A638 Gr.660, aged, room temperature
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | 660 MPa min | Aged, RT (Gr.660) |
| Yield Strength (0.2% offset) | 510 MPa min | Aged, RT |
| Elongation | 25% min | Aged, RT |
| Density | 7.94 g/cm³ | Physical |
Applicable Standards & Product Forms
Incoloy A-286 · UNS S66286 · GB/T GH2132
| Standard | Product Form |
|---|---|
| AMS 5731 | Bar & forgings (solution treated) |
| AMS 5737 | Bar (aged) |
| ASTM A453 | Bolting (Gr.660) |
| ASTM A638 | Plate, Sheet & Strip |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Incoloy Grades
Rated 650°C, in the same class as this grade, also used for fasteners, same Incoloy series.
Rated 540°C, lower than this grade, same Incoloy series.
Rated 1100°C, higher than this grade, same Incoloy series.
Rated 1100°C, higher than this grade, same Incoloy series.
Related Nickel Alloys
Rated 700°C, in the same class as this grade, also used for fasteners, from the Inconel series.
Rated 815°C, higher than this grade, also used for automotive, from the Nimonic series.
Rated 650°C, in the same class as this grade, also used for fasteners, from the Inconel series.
Pricing
How Incoloy A-286 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
What can be stated precisely is the nickel floor: at 24% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Incoloy A-286 is about USD 3.67. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Incoloy A-286 FAQWhat is Incoloy A-286 used for?
Incoloy A-286 is a Incoloy alloy used in Automotive turbocharger springs, Aircraft engine fasteners, Gas turbine discs and blades. It offers Precipitation-hardenable to high strength and Cost-effective vs Inconel grades.
What is the chemical composition of Incoloy A-286?
Incoloy A-286 is a controlled-composition Incoloy alloy supplied to AMS 5731 and AMS 5737. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Incoloy A-286 available in?
Incoloy A-286 is regularly supplied in Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet, Strip. Custom forms and dimensions available on request.
What is the maximum service temperature of Incoloy A-286?
Incoloy A-286 is rated for service up to 700°C. Contact our metallurgy team for specific application recommendations.