Inconel X-750
Precipitation-hardenable Ni-Cr alloy with excellent relaxation resistance for high-temperature springs and fasteners.
Introduction
§01, GeneralSprings that hold their preload. X-750 combines precipitation-hardened strength with relaxation resistance at temperature, which is what a spring or bolt actually needs in 700°C-class duty. Aerospace and nuclear hardware keep this 8.28 g/cm³ alloy in constant demand.
Cross-Reference
Quick Facts
- UNS
- N07750
- GB
- GH4145
- Density
- 8.28 g/cm³
- Max Service Temp
- 700°C
- Series
- Inconel
Chemical Composition
AMS 5667 / ASTM B637 (N07750), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | 70.0 min (with Co) | Base matrix |
| Chromium | Cr | 14.0 – 17.0 | Oxidation resistance |
| Iron | Fe | 5.0 – 9.0 | Controlled addition |
| Niobium + Tantalum | Nb+Ta | 0.7 – 1.2 | γ′/γ″ strengthening |
| Aluminum | Al | 0.4 – 1.0 | γ′ strengthening |
| Titanium | Ti | 2.25 – 2.75 | γ′ strengthening |
| Carbon | C | 0.08 max | Controlled residual |
| Copper | Cu | 0.5 max | Controlled residual |
Mechanical & Physical Properties
Manufacturer datasheet, typical (aged bar)
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | ≈1050 MPa | Typical, aged bar RT |
| Yield Strength (0.2% offset) | ≈725 MPa | Typical, aged bar RT |
| Elongation | ≈20% | Typical, aged bar RT |
| Density | 8.28 g/cm³ | Physical |
| Melting Range | 1395–1425 °C | Physical |
Applicable Standards & Product Forms
Inconel X-750 · UNS N07750 · GB/T GH4145
| Standard | Product Form |
|---|---|
| AMS 5667 | Bar (aged) |
| AMS 5698 | Wire |
| ASTM B637 | Bar & forgings (high temp) |
| UNS N07750 | Cross-reference designation |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Inconel Grades
Rated 650°C, in the same class as this grade, also used for fasteners, same Inconel series.
Rated 704°C, in the same class as this grade, also used for turbine, same Inconel series.
Rated 1095°C, higher than this grade, also used for generator, same Inconel series.
Rated 1100°C, higher than this grade, also used for generator, same Inconel series.
Related Nickel Alloys
Rated 700°C, in the same class as this grade, also used for fasteners, from the Incoloy series.
Rated 870°C, higher than this grade, also used for fasteners, from the Waspaloy series.
Rated 815°C, higher than this grade, also used for turbine, from the Nimonic series.
Pricing
How Inconel X-750 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
What can be stated precisely is the nickel floor: at 70% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Inconel X-750 is about USD 10.72. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Inconel X-750 FAQWhat is Inconel X-750 used for?
Inconel X-750 is a Inconel alloy used in Gas turbine hot-section springs, Nuclear reactor core springs, Aircraft engine fasteners. It offers Precipitation-hardenable to high strength and Excellent relaxation resistance to 700°C.
What is the chemical composition of Inconel X-750?
Inconel X-750 is a controlled-composition Inconel alloy supplied to AMS 5667 and AMS 5698. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Inconel X-750 available in?
Inconel X-750 is regularly supplied in Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet, Strip. Custom forms and dimensions available on request.
What is the maximum service temperature of Inconel X-750?
Inconel X-750 is rated for service up to 700°C. Contact our metallurgy team for specific application recommendations.