Inconel 718 flat product is stocked from 0.5 mm to 80 mm thick and up to 2,000 mm wide, and the gauge you choose is a design decision with three consequences: the mass you are buying, the standard the certificate cites, and the condition the mill ships. This guide gives the exact weight of a square metre at the working gauges, computed from the verified 8.19 g/cm³ density, so every figure is arithmetic rather than a table transcription, and the ordering lines that follow from it.
The stocked 718 flat-product envelope
| Parameter | Verified stock range |
|---|---|
| Thickness | 0.5-80 mm |
| Width | up to 2,000 mm |
| Condition | Hot rolled + solution annealed, pickled or 2B finish |
| Typical use | Pressure vessels, heat exchangers, reactor internals |
Gauges inside that envelope are stock items, outside it, the enquiry shifts to a mill order. The lighter gauges behave like sheet (they form and bend), while the heavier ones behave like plate (machined and welded into pressure boundaries). Both come from the same heat, but not from the same rolling practice, which is why the standard and the sampling requirement follow the gauge.
Weight per square metre by thickness
A square metre of Inconel 718 at t mm thick weighs 8.19 × t kg, because the verified density is 8.19 g/cm³. At the working gauges, and for the common 1,000 × 2,000 mm sheet:
| Thickness | Weight per m² | Weight per 1 × 2 m sheet |
|---|---|---|
| 1 mm | 8.19 kg/m² | 16.4 kg |
| 2 mm | 16.38 kg/m² | 32.8 kg |
| 3 mm | 24.57 kg/m² | 49.1 kg |
| 5 mm | 40.95 kg/m² | 81.9 kg |
| 6 mm | 49.14 kg/m² | 98.3 kg |
| 10 mm | 81.9 kg/m² | 163.8 kg |
| 12 mm | 98.28 kg/m² | 196.6 kg |
| 16 mm | 131.04 kg/m² | 262.1 kg |
| 20 mm | 163.8 kg/m² | 327.6 kg |
| 25 mm | 204.75 kg/m² | 409.5 kg |
| 40 mm | 327.6 kg/m² | 655.2 kg |
| 80 mm | 655.2 kg/m² | 1310.4 kg |
The weight column is exact, geometry times a verified density, nothing sourced or estimated. That is what makes a plate or sheet enquiry checkable: the mill’s mass figure has to reproduce this column, and any variance is a dimension or a density question, not a rounding question. Compute any other size with the weight calculator by grade and form.
Thickness decides the standard and the condition
Flat product is governed by the form-specific specification, not the bar specification. AMS 5596 covers Alloy 718 sheet, strip and plate; ASTM B670 is its industrial counterpart. Neither is interchangeable on the paper trail with AMS 5662, which covers bar, forgings and rings, the alloy is identical, the product form and its sampling requirements are not. Condition follows the gauge and the duty: flat product is normally solution heat treated as supplied, and an aged condition is stated where the drawing requires it. Thin material also carries requirements a bar specification never mentions, thickness tolerance and flatness, surface finish and sampling location, which is the practical reason the certificate must cite the flat-product standard.
Choosing the gauge: three levers
Gauge selection is decided by three things, in order:
- Structural section: the thickness that carries the load at temperature, which is a design calculation against the grade’s strength at the service temperature.
- Corrosion allowance: 718 is a strength alloy, but where the medium it tolerates is present, the allowance sets a floor on thickness and therefore on mass.
- Formability: thin gauges bend and form to tighter radii, heavier plate is machined and welded. A part that has to be formed is a different gauge from an identical part that is machined.
Fix those three before pricing, because buying a heavier gauge than the design needs adds mass and cost to the whole structure, and buying a lighter one than the load allows cannot be corrected later.
Order 718 sheet by the numbers
State the requirement in full so the certificate can be checked against it:
- Grade and identity: Alloy 718, UNS N07718.
- Form and standard: sheet, strip or plate against AMS 5596 (aerospace) or ASTM B670 (industrial).
- Dimensions: thickness in mm, width and length, inside the 0.5-80 mm × 2,000 mm envelope for stock.
- Condition: solution heat treated as supplied, and whether an aged condition is required.
- Certificate: EN 10204 3.1 heat chemistry against the cited standard; 3.2 where a third party witnesses.
Add the acceptance tests the drawing calls out, and use the RFQ spec writer to assemble them, see the 718 price per kg page for the indicative band to sanity-check a quote.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
What thicknesses of Inconel 718 sheet are stocked?
The verified stock range on this site is 0.5 mm to 80 mm thick, in widths up to 2,000 mm, supplied hot rolled and solution annealed with a pickled or 2B finish. Gauges outside that envelope move to a mill order.
How much does a square metre of 718 weigh?
A square metre weighs 8.19 × thickness in mm kilograms, because the verified density is 8.19 g/cm³. At 1 mm it is 8.19 kg/m², at 10 mm, 81.9 kg/m², at 40 mm, 327.6 kg/m². The figures are exact arithmetic from geometry and density.
Which standard covers 718 sheet and plate?
AMS 5596 for aerospace sheet, strip and plate, and ASTM B670 for the industrial equivalent. Both are flat-product specifications; AMS 5662, which many enquiries quote by habit, covers bar, forgings and rings and is not the standard a plate certificate should cite.
Is 718 sheet normally supplied aged?
No, flat product is normally supplied solution heat treated, and the aged condition is stated where the drawing requires it. Because the ageing cycle changes the sheet’s properties and its straightness, naming the condition on the purchase order is what lets the certificate prove the state you receive.