Do you need the aged strength of a disc alloy to 650 °C, or the weldable corrosion armour of a solid-solution Ni-Cr-Mo to 980 °C?

Inconel 718 is a precipitation-hardenable nickel-chromium alloy with outstanding strength, corrosion resistance and fabricability.

Route the decision

  • If the part is a turbine disc, ring, bolt or subsea wellhead component that must carry load, take Inconel 718: precipitation-hardened to 38 HRC, verified 1275 MPa tensile at room temperature and still 860 MPa at 650 °C.
  • If the part is welded hardware facing seawater, acids or sour gas, piping, risers, ducting, take Inconel 625: verified pitting and crevice-corrosion resistance, excellent weldability, NACE MR0175 for sour service, oxidation resistance to 980 °C.
  • If the duty is a welded assembly under load below 650 °C, Inconel 718 can be welded and aged, but the corrosion-chemistry callout belongs to 625, and weld-overlay practice is built around it.
  • If temperature above 650 °C decides, Inconel 625 is the only one of the pair still inside its verified envelope, and Inconel 718’s datasheet guarantee ends at its 650 °C ceiling.

As a concrete pairing: a subsea completion: the wellhead body and its hangers are Inconel 718 forgings carrying load at temperature, while the clamp piping and umbilical terminations around them are welded Inconel 625 resisting the seawater the forgings are coated against. One system, two alloys.

PropertyInconel 718Inconel 625
UNS / GBN07718N06625
Density8.19 g/cm³8.44 g/cm³
Max service temp650 °C980 °C
Governing standardsAMS 5662, AMS 5663, ASTM B637, UNS N07718ASTM B443, ASTM B444, ASTM B446, AMS 5666, NACE MR0175
Stock formsForging, Wire, Spring Wire, Bar, Plate, StripForging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube

Specification signals

Inconel 718 wins on load-bearing at temperature: 1035 MPa yield aged to 38 HRC, usable strength to 650 °C, and the AMS 5662/5663 rotating-quality trail discs and fasteners are audited against. Inconel 625 wins on environment and fabrication: pitting, crevice and stress-corrosion resistance verified, non-magnetic, oxidation to 980 °C, and the weldability that makes it a standard piping and overlay alloy under ASTM B443/B444/B446.

  • Inconel 718: Inconel 718 wins on load-bearing at temperature: 1035 MPa yield aged to 38 HRC, usable strength to 650 °C, and the AMS 5662/5663 rotating-quality trail discs and fasteners are audited against.
  • Inconel 625: Inconel 625 wins on environment and fabrication: pitting, crevice and stress-corrosion resistance verified, non-magnetic, oxidation to 980 °C, and the weldability that makes it a standard piping and overlay alloy under ASTM B443/B444/B446.

Switch triggers

Move Inconel 625 to Inconel 718 when static corrosion hardware becomes load-bearing below 650 °C and the AMS audit trail is required, and move Inconel 718 to Inconel 625 the moment welding dominates the fabrication or the temperature passes 650 °C.

What the choice costs, and why no band is printed here

The two grades are both priced off the nickel market, but they do not carry the same alloy content: 625 runs about 58 % nickel with 8-10 % molybdenum, while 718 runs about 50-55 % nickel with only 2.8-3.3 % molybdenum and no tungsten. Molybdenum is the expensive element in that comparison, so 625 carries a premium purely on alloy content — while 718 carries a different premium, on process, because it needs a two-step ageing cycle that 625 does not.

Neither premium is stable enough to publish as a per-kilogram band. The alloy charge moves with the nickel index weekly, and the ageing cost depends on lot size. What is stable is the ordering:

Compare onHigher costWhy
Alloy content, same formInconel 6258-10 % molybdenum against 718’s 2.8-3.3 %
Finished part, aged conditionInconel 718Solution plus two-step age, tested per lot
Seamless tube against barBoth gradesPiercing and cold drawing, not alloy

The two premiums can cancel out or stack depending on what you are buying: a solution-treated 625 bar and a black 718 bar can land close together, while 718 aged to AMS 5662 can sit above an annealed 625 bar of the same section. That is why comparing grade to grade without comparing condition is the mistake that costs money — the mechanism is worked through on the 718 price page and the 625 price page.

Compute the mass with the weight calculator first. Mass is the only figure in this comparison that is exact.

Part-selection matrix, grade by component

Where the decision is made in practice, component by component:

ComponentGradeWhy
Turbine disc, ring or shaft below 650 °CInconel 718Aged strength to 38 HRC with the AMS 5662/5663 rotating-quality trail
Turbine disc or ring between 650 and 870 °Cneither, Waspaloy718’s datasheet guarantee ends at 650 °C. Waspaloy holds creep-rupture strength across the band
Subsea wellhead body, hanger, hanger fastenerInconel 718Listed verified application, the fastener-grade strength envelope 625 does not carry
Umbilical clamp piping, riser termination, welded seawater lineInconel 625Weldability plus pitting and crevice resistance, with NACE MR0175 for sour service
Weld overlay or clad layer on carbon steelInconel 625The industry’s standard overlay alloy, the weld-chemistry callout is built around it
Bellows, diaphragm, expansion jointInconel 625Solid-solution ductility and clean weldability at thin gauge
Springs and fasteners at temperatureInconel 718Spring wire is a stocked form and the aged hardness is what a fastener needs
Combustion-zone liner above 650 °Cneither, Hastelloy XOxidation resistance verified to 1100 °C

The matrix reads in one direction: load below 650 °C goes to 718, welded chemistry goes to 625, and the two rows that say “neither” are the real traps: the hot disc and the combustion liner each leave the pair entirely. If your duty is a pair you cannot see here, run it through the selection wizard grade-level comparison, which routes two named grades against each other from the verified data.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

Inconel 718 or Inconel 625 for a subsea fastener?

Inconel 718, subsea wellhead components are listed verified applications, and its aged strength (1035 MPa yield at 38 HRC) is what a fastener needs. Both grades resist sour service, and only 718 carries the fastener-grade strength envelope.

Which of the two welds more easily?

Inconel 625, excellent weldability is a verified key feature and it is the industry’s overlay standard. Inconel 718 welds but its aged condition means weld zones need the aging treatment re-considered.

Which runs hotter, 718 or 625?

Inconel 625, by a wide margin: 980 °C oxidation resistance verified against Inconel 718’s 650 °C ceiling, though 625 is solid-solution and will not match 718’s aged strength at any temperature.

Are Inconel 718 and 625 interchangeable?

No. One is an age-hardenable strength alloy, the other a solid-solution corrosion alloy. Load-bearing hardware below 650 °C routes to 718, and welded corrosion hardware routes to 625.

Which is more expensive, Inconel 718 or Inconel 625?

Inconel 625, on alloy content: about 58 % nickel with 8-10 % molybdenum against 718’s roughly 50-55 % nickel with about 3 % molybdenum. On the indicative 2026 bar band that puts 625’s mid-band around 26 % above 718’s. These are market reference bands from public price guides, not quotations, and both float with LME nickel and certification level.

Can I substitute 625 for 718 to save weight or cost?

No. The premium runs the other way, 625 costs more because of its molybdenum content, and the two do different jobs: 718 is the age-hardened strength grade to 650 °C, 625 is the solid-solution corrosion and weldability grade to 980 °C. Substituting either direction loses the property it was chosen for.