Process reference

Verified heat-treatment cycles

The 3 heat-treatment cycles this site documents step by step, each with its target property and the page that carries the full anchor. Other precipitation-hardened grades (Incoloy 925) are honestly marked not covered.

Inconel 718

precipitation-hardened
  1. 1 Solution treat 954-968 °C, ~1 h, air cool
  2. 2 First age 718 °C / 8 h
  3. 3 Furnace cool ~55 °C/h to 621 °C
  4. 4 Second age 621 °C / ≥8 h, air cool

Target: 38 HRC with 1275 MPa UTS

Full cycle detail and anchors →

Nimonic 80A

precipitation-hardened
  1. 1 Solution 1080 °C / 8 h
  2. 2 Age 700 °C / 16 h

Target: γ′ strengthening for valve and spring duty to 815 °C

Full cycle detail and anchors →

Waspaloy

precipitation-hardened
  1. 1 Solution treatment in the 1010-1040 °C band per the site process page
  2. 2 Stabilise, then age in two steps

Target: creep-rupture bandwidth 650-870 °C

Full cycle detail and anchors →

Frequently Asked Questions (FAQ)

Why does this table only list three grades?

Because a heat-treatment cycle published without a verifiable anchor is worse than no cycle. These three cycles are the ones this site documents with full step-by-step detail on dedicated pages, Inconel 718 from its heat-treatment page, Nimonic 80A and Waspaloy from the heat-treatment guide and process pages. The other grades are listed as honestly not covered rather than padded with generic numbers.

What does a double-age cycle actually do?

The first age at the higher temperature nucleates the strengthening precipitate (γ″ in 718); the furnace cool and the second, lower age grow it to the size that delivers the hardness-and-toughness combination. Skipping the second age leaves strength on the table; running both steps too hot trades toughness for hardness.

Can I run this cycle on a part I already bought?

Only after you know the delivered condition. Bar ordered to AMS 5663 arrives already solution-treated and aged, re-running the full cycle can coarsen the structure. Check the certificate condition first, then heat treat only what the specification calls for.

Need the cycle for a grade not listed?

Tell us the grade and the duty, we confirm what the governing standard requires, state what is documented and what is not, and quote material in the right delivered condition.

Send your requirement