5 of the 20 stocked grades carry a NACE MR0175 sour-service qualification in their verified standard list: with API 6A flagged where the wellhead-level document applies too.
A solid-solution Ni-Cr-Mo alloy that keeps both strength and corrosion resistance from cryogenic to 980 °C.
The Ni-Cu workhorse for seawater and hydrofluoric acid, non-magnetic with good properties to 540 °C.
The fine-grain 800H variant optimized for hot forming with the 800 family's high-temperature strength and corrosion resistance.
The Ni-Fe-Cr-Mo-Cu grade with outstanding sulfuric and phosphoric acid resistance and NACE sour qualification.
The age-hardenable Ni-Fe-Cr grade with API 6A wellhead qualification for sour gas hardware.
It is the environmental-crackability layer for H₂S service: hardness ceilings, chemistry and heat-treatment-condition limits that keep the alloy out of sulphide stress cracking territory. It rides on top of the mill standard, an ASTM document for the grade plus MR0175 qualification for the duty, and both belong on the purchase specification.
API 6A is the wellhead and Christmas-tree equipment standard, it adds the equipment-level requirements (pressure classes, PSL, test regimes) on top of MR0175's material-level limits. 925 is the age-hardenable member of the Ni-Fe-Cr family qualified for that hardware; 825 covers the non-ageing corrosion-duty roles in the same wells.
No. MR0175 qualification is condition-specific: an age-hardenable grade outside its qualified heat-treatment condition, or a cold-worked condition beyond the hardness limit, can fall out of scope. The certificate condition matters as much as the grade name, which is why the purchase spec should name both.
Send the H₂S partial pressure, temperature and the component, we confirm the qualified grade and condition pair and quote against NACE MR0175 with the certificate.
Send your requirement