The verified weldability statement for each of the 20 stocked grades: from Inconel 718's documented weldability to C-276's no-post-weld-heat-treatment route: with the matching AWS A5.14 filler where one is documented, and honest flags where no claim is.
| Alloy | Verified weldability statement | Post-weld heat treatment | AWS A5.14 filler | Joining notes |
|---|---|---|---|---|
| Inconel 718N07718 | Excellent fabricability and weldability | Not documented for this grade. | ERNiFeCr-2 | , |
| Inconel 625N06625 | Excellent weldability | Not documented for this grade. | ERNiCrMo-3 | , |
| Hastelloy C-276N10276 | Good weldability without post-weld heat treatment | No post-weld heat treatment required (verified feature). | ERNiCrMo-4 | , |
| Hastelloy XN06002 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | ERNiCrMo-2 | , |
| Monel 400N04400 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | ERNiCu-7 | , |
| Nimonic 80AN07080 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| WaspaloyN07001 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| Nickel 200N02200 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| MP35NR30035 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| L605R30605 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| 4J29, | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | Good plating and brazing |
| 4J36, | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| 1J22, | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| 1J50, | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| Incoloy 800N08800 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | ERNiCr-3 | , |
| Incoloy 800HN08810 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| Incoloy 800HTN08811 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| Incoloy 825N08825 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| Incoloy 925N09925 | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
| 3J21, | No weldability claim in the verified feature set, qualify the procedure against the datasheet. | Not documented for this grade. | , | , |
Filler selection, post-weld rules and dissimilar-joint logic: welding consumables matching · weldability hub · verified heat-treatment cycles
Exactly what it says: the grade's verified feature set on this site documents no weldability claim. That is not a verdict against welding, it means the weld procedure (filler, preheat, post-weld heat treatment) must be qualified against the grade datasheet before fabrication, rather than assumed from a marketing line.
Because it is the documented exception: Hastelloy C-276 verifies good weldability without post-weld heat treatment, which is what makes as-welded vessel construction viable in the low-carbon C family.
4J29 verifies good plating and brazing, the joining routes that matter for hermetic glass-to-metal packages, where brazing rather than fusion welding is the process.
The AWS A5.14 bare-wire classification system, ERNiFeCr-2 for Alloy 718, ERNiCrMo-3 for 625, ERNiCrMo-4 for C-276 and so on. The pairing page carries the full table with the weld-metal behaviour and the post-weld rule each class implies.
Send the joint design and duty. We reply with the grade, condition and the certificate that proves the heat before and after the weld.
Send your requirement