A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.

As strength anchors from the verified feature sets, MP35N achieves over 1800 MPa tensile while staying non-magnetic per ASTM F562, and Nimonic 80A carries gamma-prime strengthening with service to 815 °C.

What this page covers

Working route follows form: hot working for rings, discs and shafts, cold working for wire and strip. At RAS Thermal forgings run from 5 kg to 3,000 kg (ring-rolled, upset and open-die), wire is cold drawn to Ø0.10-12.0 mm, strip is cold rolled to spring temper or soft. The certificate states the final condition.

The verified numbers

Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). Hot working: forging 5-3,000 kg. Cold working: wire Ø0.10-12.0 mm. Strip: spring temper or soft. Proof: condition on certificate.

What this means for your selection

Working route follows form: hot working for rings, discs and shafts, cold working for wire and strip. At RAS Thermal forgings run from 5 kg to 3,000 kg (ring-rolled, upset and open-die), wire is cold drawn to Ø0.10-12.0 mm, strip is cold rolled to spring temper or soft. The certificate states the final condition. The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.

How the candidate options compare

  • Bar & Rod: Ø6-350 mm · length to 6,000 mm, and typical use: Machined valve trim, fasteners, pump shafts, downhole tools.
  • Plate & Sheet: Thk. 0.5-80 mm · width to 2,000 mm, and typical use: Pressure vessels, heat exchangers, reactor internals.
  • Strip: Thk. 0.05-3.0 mm · width 4-600 mm, and typical use: Bellows, diaphragms, magnetic cores, sealing rings.
  • Pipe & Tube: OD 6-219 mm · wall 0.5-20 mm, and typical use: Umbilical lines, condenser tubing, chemical piping.
  • Wire: Ø0.10-12.0 mm in coil, spool or cut-to-length, and typical use: Springs, fasteners, welding consumables, sensors.
  • Forging: Ring-rolled, upset and open-die from 5 kg to 3,000 kg, and typical use: Turbine discs, flanges, shafts, rings.
  • Flange: ASME B16.5 / B16.47 in Class 150 through 2500, and typical use: Piping systems, pressure vessels, skids.

Follow the links for the per-grade pages, the figures there match the ones on this page.