Nimonic Series
Ni-Cr-Ti and Ni-Cr-Co age-hardenable alloys developed for gas turbine hot-section components and high-temperature springs.
About Nimonic Series
Nimonic Series is a series of nickel-base alloys. Ni-Cr-Ti and Ni-Cr-Co age-hardenable alloys developed for gas turbine hot-section components and high-temperature springs. The series currently covers 4 grades, supplied as Forging, Wire, Spring Wire, Bar & Rod, Plate & Sheet to BS HR 1, BS HR 2, ASTM B637, AMS 5540 requirements. Orders ship with 100% heat-traceable mill test certification, and technical enquiries receive a substantive reply within 24 hours.
Where This Series Fits
- Strengthened primarily by γ′ precipitates (nickel-titanium-aluminium), balancing high-temperature strength with oxidation resistance
- Nimonic 80A is the classic material for automotive and marine diesel engine exhaust valves
- Nimonic 90 adds cobalt to raise the γ′ solvus temperature, with creep strength serviceable up to about 920°C
- Nimonic 901 is iron-nickel-chromium base, balancing creep strength with forgeability for turbine discs and ring components
Available Forms
Applicable Standards
Nimonic Series: Grade Comparison
4 grades| Grade | Max service temp | Density | Typical use |
|---|---|---|---|
| Nimonic 75 | 1000 °C | 8.37 g/cm³ | Ni-Cr-Ti alloy for sheet metal combustion components and heat-treatment fixtures. |
| Nimonic 80A | 815 °C | 8.19 g/cm³ | Ni-Cr-Ti-Al alloy for exhaust valves, turbine blades and high-temperature springs. |
| Nimonic 90 | 920 °C | 8.18 g/cm³ | Age-hardenable Ni-Cr-Co alloy for turbine blades and high-temperature springs to 920°C. |
| Nimonic 901 | 750 °C | 8.2 g/cm³ | Ni-Fe-Cr alloy for turbine discs and rings with balanced creep strength and forgeability. |
Frequently Asked Questions (FAQ)
What is the Nimonic Series?
Nimonic Series is a series of nickel-base alloys. Ni-Cr-Ti and Ni-Cr-Co age-hardenable alloys developed for gas turbine hot-section components and high-temperature springs. RAS Thermal supplies 4 grades in this series.
What standards apply to Nimonic Series materials?
Supply follows BS HR 1, BS HR 2, ASTM B637, AMS 5540, with the mill test certificate referencing the exact designation called out on your purchase order.
How do I request a quote for Nimonic grades?
Send the grade, form, dimensions, standard and quantity, our metallurgy team replies within 24 hours with availability, pricing and a sample mill test certificate on request.